Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 6015 Phenolic, Briquette, Transfer Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Mineral/Glass Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 6015 Phenolic, Briquette, Transfer Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 06015 is a glass and mineral filled phenolic molding compound offering improved mechanical strength, dimensional stability and excellent electrical properties. 06015 is available in black.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.630 g/cc
0.0228 lb/in³
ASTM D1895
Density 1.72 g/cc
0.0621 lb/in³
ASTM D792
Water Absorption 0.078 %
0.078 %
ASTM D570
Linear Mold Shrinkage 0.00090 cm/cm
0.00090 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 94
94
ASTM D785
Tensile Strength, Ultimate 101 MPa
14600 psi
ASTM D638
Elongation at Break 0.84 %
0.84 %
ASTM D638
Tensile Modulus 15.3 GPa
2220 ksi
ASTM D638
Flexural Strength 163 MPa
23600 psi
ASTM D790
Flexural Modulus 15.1 GPa
2190 ksi
ASTM D790
Compressive Strength 215 MPa
31200 psi
ASTM D695
Poissons Ratio 0.31
0.31
ASTM D638
Shear Modulus 5.84 GPa
847 ksi
Calculated
Izod Impact, Notched 0.440 J/cm
0.824 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.450 J/cm²
2.14 ft-lb/in²
ASTM D256
Impact 206
206
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 49.0 µm/m-°C

@Temperature 40.0 - 130 °C
27.2 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Maximum Service Temperature, Air 236 °C
457 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 279 °C
534 °F
ASTM D648
Flammability, UL94 V-1

@Thickness 3.10 mm
V-1

@Thickness 0.122 in
Shrinkage 0.056 %
0.056 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+12 ohm-cm
2.00e+12 ohm-cm
ASTM D247
Dielectric Constant 5.0
5.0
ASTM D150
Dielectric Strength 11.5 kV/mm
292 kV/in
Step by Step; ASTM D149
16.3 kV/mm
414 kV/in
Short Time; ASTM D149
Dissipation Factor 0.028
0.028
ASTM D150
Arc Resistance 184 sec
184 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638
Users viewing this material also viewed the following: