Material Notes:
1 part resin to 1 part hardener.TIGA 101-EX is an exceptional epoxy formulation, recommended for lower temperature or wet industrial bonding applications where fast curing is required. This clear, two-part, mild odor, medium- viscosity system mixes easily at room temperature, contains no solvents, and is suitable for high performance structural-bonding applications where the combination of very fast room temperature cure coupled with low shrinkage and excellent mechanical and electrical properties is required. It develops strong, tough bonds to metals, phenolic plastics, polyesters, glass and glass fabrics, hardboards and forestry products, ceramics, rubber, masonry materials, and other construction materials. Fully cured TIGA 101-EX is an excellent electrical insulator and provides superior resistance to vapors and gases, water, galvanic action, petroleum fuels, salt solutions, and many other organic and inorganic compounds.Applications: High speed bonding and repairs at low temperatures. Ideal for assembly lines and various production applications such as staking, fillet bonds, and general industrial repairs. Used in component assembly, appliances, electronics, and fiber optics. Sets in five minutes, reaches full strength in about one hour.Information provided by Resin Technology Group.
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
Of resin
Viscosity 10000 - 16000 cP
10000 - 16000 cP
Of hardener at 25C
11000 - 15000 cP

@Temperature 25.0 °C
11000 - 15000 cP

@Temperature 77.0 °F
Of resin
14000 - 17000 cP

@Temperature 25.0 °C
14000 - 17000 cP

@Temperature 77.0 °F
Mixed
Mechanical Properties Metric English Comments
Hardness, Shore D 28
28
Cured 10 minutes at 25°C
68
68
Cured 30 minutes at 25°C
74
74
Cured 10 minutes at 60°C
78 - 82
78 - 82
Shear Strength 15.2 - 22.1 MPa
2200 - 3200 psi
Lap
Izod Impact, Notched 1.12 J/cm
2.10 ft-lb/in
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 125 °C
257 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 16.3 kV/mm
415 kV/in
Processing Properties Metric English Comments
Pot Life 3.0 - 5.0 min
3.0 - 5.0 min
Small Mass
Descriptive Properties Value Comments
Color Transparent, Clear