Electrical Properties Metric English Comments
Dielectric Strength 6.50 kV/mm
165 kV/in
AC 60 Hz
Fujipoly Industries Sarcon® 20GTR Thin-Film GTR
Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of ..
Dielectric Strength 6.50 kV/mm
165 kV/in
60Hz, Step-by-Step, wet; ASTM D149
Sumitomo Bakelite North America SI 9002N-1 Silicone Compound
Short fibergass reinforced silicone molding compound which offers moderate strength properties, dimensional stability, and excellent long-term thermal stability at elevated temperatures.Information ..
Dielectric Strength 6.50 kV/mm
165 kV/in
ASTM D149
Tipco Tipcolite® TEL 211 Phenolic Compound, Glass & Nylon Fibers, Soft Flow & Low Shrinkage
Soft Flow Phenolic Compound, Reinforced with Glass & Nylon FibresApplications: Automotives & ElectricalProcessing: Compression & TransferInformation provided by the Manufacturer, Tipco Industries L..
Dielectric Strength 6.50 - 7.50 kV/mm

@Temperature 90.0 °C
165 - 191 kV/in

@Temperature 194 °F
IS 2584-1963
Amity Thermosets ATF 197 Phenolic Molding Inorganic and glass Filler, Compression Molded
Characteristics:Flame retardantSpark resistant Good electrical insulationHeat stability ( 200°C )Good mouldability Low water absorptionLow shrinkageColor-blackSoft/medium flow Applications:Switchg..
Dielectric Strength 6.50 - 8.00 kV/mm

@Temperature 90.0 °C
165 - 203 kV/in

@Temperature 194 °F
IS 2584-1963
Amity Thermosets ATS 155 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded
Characteristics:Shock resistantElectrical low lossHigh mechanical strengthHeat stableHigh electrical insulationDimensional stabilityGood mechanical tension bearing strengthGood copper adhesion Color..
Dielectric Strength 6.50 kV/mm
165 kV/in
60Hz, Step-by-Step, wet; ASTM D149
Sumitomo Bakelite North America SI 9002J-1 Silicone Compound
SI 9002J-1 is a short fiberglass reinforced silicone molding compound, which offers moderate strength properties, and dimensional stability and excellent long-term thermal stability at elevated temp..