Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 6.50 - 7.50 kV/mm @Temperature 90.0 °C |
165 - 191 kV/in @Temperature 194 °F |
IS 2584-1963 |
Amity Thermosets ATF 197 Phenolic Molding Inorganic and glass Filler, Compression Molded Characteristics:Flame retardantSpark resistant Good electrical insulationHeat stability ( 200°C )Good mouldability Low water absorptionLow shrinkageColor-blackSoft/medium flow Applications:Switchg.. |
|||
Dielectric Strength | 5.50 - 7.50 kV/mm @Temperature 90.0 °C |
140 - 191 kV/in @Temperature 194 °F |
IS 2584-1963 |
Amity Thermosets ATI 172 Phenolic Molding Organic and inorganic Filler, Injection Molded Characteristics:Heat resistant ( asbestos free )Good electric insulationLow shrinkageLow water absorptionMedium mechanical strengthNot suitable for high mechanical tensionColor-blackVery soft flow .. |
|||
Dielectric Strength | 5.50 - 7.50 kV/mm @Temperature 90.0 °C |
140 - 191 kV/in @Temperature 194 °F |
IS 2584-1963 |
Amity Thermosets ATO 142 Phenolic Molding Organic Filler, Compression Molded Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-black, brownMedium/hard flow Applications: Elec.. |