Polymer Property : Dielectric Strength = 1700 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 66.9 kV/mm
1700 kV/in
Resin Technology Group UV CC-2004 Multi-Functional, UV Curing, Conformal-Coating
Multi-functional UV-CC 2004 is a single component, solvent-less conformal-coating specifically formulated for rapid room temperature cure when exposed to UV light. Thin layer coatings cure almost in..
Dielectric Strength 66.9 kV/mm
1700 kV/in
ASTM D-149
Saint-Gobain Norton® Fluorglas® Chemfilm® R191 Skived Sintered PTFE Tape (0.010" thick)
Description: Skived Sintered PTFE Films are used as barrier and insulation tapes for wire and cable, as well as the primary wall material for convoluted hose, Description: Skived sintered films meet..
Dielectric Strength 66.9 kV/mm
1700 kV/in
ASTM D-149
Saint-Gobain Norton® T-100 Virgin Skived PTFE Film (0.010" thick)
T-100/T-200 Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate rele..
Dielectric Strength 67.0 kV/mm
1700 kV/in
Full-wave Impulse; ASTM D3426
DuPont™ Nomex® 418 Paper, 10 mil Nominal Thickness
Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen..
Dielectric Strength 66.9 kV/mm
1700 kV/in
ASTM D149
Arkema Group KYNAR® 710, 710 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Dielectric Strength 66.9 kV/mm
1700 kV/in
ASTM D149
Arkema Group KYNAR® 740 Black/Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistance; high purityAppli..
Dielectric Strength 66.9 kV/mm
1700 kV/in
ASTM D149
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Dielectric Strength 66.9 kV/mm
1700 kV/in
ASTM D149
Arkema Group KYNAR® 740-02 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mecha..
Dielectric Strength 66.9 kV/mm
1700 kV/in
ASTM D149
Arkema Group KYNAR® 760 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Dielectric Strength 66.9 kV/mm
1700 kV/in
ASTM D149
3M 7957MP Hi-Performance Acrylic 200MP
This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia..
Dielectric Strength 66.9 kV/mm
1700 kV/in
ASTM D149
3M 7993MP Hi-Performance Acrylic 200MP
This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia..
Dielectric Strength 66.9 kV/mm
1700 kV/in
ASTM D149
3M 7995MP Hi-Performance Acrylic 200MP
This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia..
Dielectric Strength 66.9 kV/mm
1700 kV/in
ASTM D149
Arkema Group KYNAR® 720, 720 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Dielectric Strength 66.9 kV/mm
1700 kV/in
ASTM D149
3M 7956MP Hi-Performance Acrylic 200MP
This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia..
Dielectric Strength 66.9 kV/mm
1700 kV/in
ASTM D149
3M 7997MP Hi-Performance Acrylic 200MP
This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia..
Dielectric Strength 66.9 kV/mm
1700 kV/in
ASTM D149
3M 9056MP Hi-Performance Acrylic 200MP
This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia..
Dielectric Strength 66.9 kV/mm
1700 kV/in
ASTM D149
3M 9057MP Hi-Performance Acrylic 200MP
This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia..
Dielectric Strength 66.9 kV/mm
1700 kV/in
Saint-Gobain CHR® 2045-10 Skived PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape
Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu..