Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 25.6 - 40.0 kV/mm | 650 - 1020 kV/in | Average value: 33.3 kV/mm Grade Count:6 |
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled". Specific grades with glass content between 15% an.. |
|||
Dielectric Strength | 25.6 kV/mm | 650 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA12 Availability: North AmericaForms: PelletsFeatures: Low ViscosityTPCI# 8807105Information provided by TP Composites, Inc. |
|||
Dielectric Strength | 25.6 kV/mm | 650 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA12 L N MB Availability: North AmericaForms: PelletsFeatures: Low ViscosityTPCI# 8807105Information provided by TP Composites, Inc. |
|||
Dielectric Strength | 25.6 kV/mm | 650 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Luriblend® PA12 TS18 Availability: North AmericaForms: PelletsAdditive: Silicone Lubricant(2%) and PTFE Lubricant(18%)Features: LubricatedInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 25.6 kV/mm | 650 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA12 E HS Availability: North AmericaForms: PelletsAdditive: Heat StabilizerFeatures: Heat StabilizedProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 25.6 kV/mm | 650 kV/in | Test run on 1/8" specimens. |
Loctite® Durabond® E-120HP Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |
|||
Dielectric Strength | 25.6 kV/mm @Thickness 1.59 mm |
650 kV/in @Thickness 0.0625 in |
|
Cytec EN-2521 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
Dielectric Strength | 25.6 kV/mm @Thickness 1.59 mm |
650 kV/in @Thickness 0.0625 in |
|
Cytec EN-2543 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
Dielectric Strength | 25.6 kV/mm | 650 kV/in | 2.03 mm; ASTM D149 |
ExxonMobil Santoprene® 121-58W175 Thermoplastic Elastomer A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed for .. |
|||
Dielectric Strength | 25.6 kV/mm | 650 kV/in | ASTM D149 |
Arlon 51599R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone RubberLayer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass Product Use: Flexible heater insulationAppearance: Red s.. |
|||
Dielectric Strength | 25.6 kV/mm | 650 kV/in | ASTM D149 |
Arlon 51866R020 0.020" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production material .. |
|||
Dielectric Strength | 25.6 kV/mm | 650 kV/in | ASTM D149 |
Arlon 55572R030 0.030" (0.762 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass Appearance: Red silicone rubber on fiberglass clothThis data Represents typical values for the production material. T.. |
|||
Dielectric Strength | 25.6 kV/mm | 649 kV/in | ASTM D149 |
Arlon T2020-R004 0.020" (0.508 mm) Cured Self-Fusing Silicone Rubber Description: 1 inch wide x 20 mil thick, Black, Triangular cross-section, Self-Fusing Silicone TapeDesign/Construction: Interleave: Polyethylene Product: Cured Self-Fusing Silicone RubberCross-Secti.. |
|||
Dielectric Strength | 25.6 kV/mm | 650 kV/in | ASTM D149 |
Arlon R37582R0055 0.0055" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 1.5 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 2113 FiberglassThis data represents typical values for the production material and should not be .. |
|||
Dielectric Strength | 25.6 kV/mm | 650 kV/in | ASTM D149 |
Arlon R37652R0055 0.0055" (0.140 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 2113 Fiberglass Appearance: Red silicone rubber on fiberglass clothThis data Represents typical values for the production material. .. |