Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 30.0 - 40.0 kV/mm | 762 - 1020 kV/in | IEC 60243-1 |
Raschig Group AMPLA® 2000 melamine-modified polyester Halogen-free, organically and inorganically filled melamine-modified Polyester molding compound. Low post-shrinkage, very good electrical values, high heat resistance, very good sliding behavior, ve.. |
|||
Dielectric Strength | 30.0 - 40.0 kV/mm | 762 - 1020 kV/in | IEC 60243-1 |
Raschig Group AMPLA® 7500 melamine-modified polyester Organically and inorganically filled melamine modified Polyester molding compound. Low post-shrinkage, very good electrical values, excellent heat resistance, very good sliding behavior and wear sta.. |
|||
Dielectric Strength | 18.9 - 40.0 kV/mm | 480 - 1020 kV/in | Average value: 25.5 kV/mm Grade Count:16 |
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi.. |
|||
Dielectric Strength | 12.2 - 40.0 kV/mm | 310 - 1020 kV/in | Average value: 16.1 kV/mm Grade Count:34 |
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled". Each property range of values repor.. |
|||
Dielectric Strength | 27.0 - 40.0 kV/mm | 686 - 1020 kV/in | Average value: 31.3 kV/mm Grade Count:11 |
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi.. |
|||
Dielectric Strength | 25.6 - 40.0 kV/mm | 650 - 1020 kV/in | Average value: 33.3 kV/mm Grade Count:6 |
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled". Specific grades with glass content between 15% an.. |
|||
Dielectric Strength | 20.0 - 40.0 kV/mm @Temperature 100 - 200 °C |
508 - 1020 kV/in @Temperature 212 - 392 °F |
Average value: 27.6 kV/mm Grade Count:3 |
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an.. |
|||
Dielectric Strength | 20.0 - 40.0 kV/mm @Thickness 0.800 - 3.20 mm |
508 - 1020 kV/in @Thickness 0.0315 - 0.126 in |
Average value: 27.6 kV/mm Grade Count:3 |
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an.. |
|||
Dielectric Strength | 18.9 - 40.0 kV/mm | 480 - 1020 kV/in | Average value: 25.7 kV/mm Grade Count:5 |
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl.. |
|||
Dielectric Strength | 15.7 - 40.0 kV/mm | 400 - 1020 kV/in | Average value: 24.5 kV/mm Grade Count:33 |
Overview of materials for Nylon 66, Glass/Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Dielectric Strength | 35.0 - 40.0 kV/mm | 889 - 1020 kV/in | Average value: 37.5 kV/mm Grade Count:4 |
Overview of materials for Nylon 12, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Dielectric Strength | 20.0 - 40.0 kV/mm @Thickness 2.00 mm |
508 - 1020 kV/in @Thickness 0.0787 in |
IEC 60243 |
Manifattura Cattaneo PVC HI Polyvinyl Chloride Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Dielectric Strength | 20.0 - 40.0 kV/mm @Thickness 2.00 mm |
508 - 1020 kV/in @Thickness 0.0787 in |
IEC 60243 |
Manifattura Cattaneo PVC U Polyvinyl Chloride Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Dielectric Strength | 20.0 - 40.0 kV/mm | 508 - 1020 kV/in | ASTM D149/15 |
Mikro-Technik Reproflon PTFE Reproflon is reclaimed PTFE scraps. The powder can be reused for the usual manufacturing procedures.Information provided by Mikro-Technik GmbH |
|||
Dielectric Strength | 35.0 - 40.0 kV/mm @Thickness 1.00 mm |
889 - 1020 kV/in @Thickness 0.0394 in |
ASTM D149 |
Solvay Specialty Polymers Hyflon® MFA® F1530 Perfluoropolymer Hyflon® MFA is a family of perfluoro polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame resistanc.. |
|||
Dielectric Strength | 35.0 - 40.0 kV/mm | 889 - 1020 kV/in | ASTM D149 |
Solvay Specialty Polymers Hyflon® PFA 420 Perfluoroalkoxy (PFA) Hyflon® PFA is a family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resistance.. |
|||
Dielectric Strength | 35.0 - 40.0 kV/mm | 889 - 1020 kV/in | ASTM D149 |
Solvay Specialty Polymers Hyflon® PFA M620 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Dielectric Strength | 35.0 - 40.0 kV/mm | 889 - 1020 kV/in | ASTM D149 |
Solvay Specialty Polymers Hyflon® PFA M640 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Dielectric Strength | 35.0 - 40.0 kV/mm | 889 - 1020 kV/in | ASTM D149 |
Solvay Specialty Polymers Hyflon® PFA P450 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Dielectric Strength | 35.0 - 40.0 kV/mm | 889 - 1020 kV/in | ASTM D149 |
Solvay Specialty Polymers Hyflon® PFA P455 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Dielectric Strength | 35.0 - 40.0 kV/mm | 889 - 1020 kV/in | ASTM D149 |
Solvay Specialty Polymers Hyflon® MFA® 1041 Perfluoropolymer Hyflon® MFA 1041 is a high extrusion speed resin specifically designed for insulation for plenum-rated LAN cables. MFA 1041 delivers superior electrical performance in addition to its excellent f.. |
|||
Dielectric Strength | 25.0 - 40.0 kV/mm | 635 - 1020 kV/in | ASTM D149 |
Adamas Adalon® 415 PTFE, 10% Organic Filler Information provided by Adamas, HPM |
|||
Dielectric Strength | 25.0 - 40.0 kV/mm | 635 - 1020 kV/in | ASTM D149 |
Adamas Adalon® 433 PTFE, 10% Ekonol® Information provided by Adamas, HPM |
|||
Dielectric Strength | 25.0 - 40.0 kV/mm | 635 - 1020 kV/in | ASTM D149 |
Adamas Adalon® 436 PTFE, 15% Ekonol® Information provided by Adamas, HPM |
|||
Dielectric Strength | 35.0 - 40.0 kV/mm | 889 - 1020 kV/in | ASTM D149 |
Solvay Specialty Polymers Hyflon® PFA M640 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista.. |
|||
Dielectric Strength | 35.0 - 40.0 kV/mm | 889 - 1020 kV/in | ASTM D149 |
Solvay Specialty Polymers Hyflon® PFA P450 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista.. |
|||
Dielectric Strength | 16.5 - 40.0 kV/mm | 420 - 1020 kV/in | Average value: 27.6 kV/mm Grade Count:6 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced". Each property range of values repo.. |
|||
Dielectric Strength | 20.0 - 40.0 kV/mm | 508 - 1020 kV/in | VDE 0303 |
GEHR Plastics PVC-U Polyvinylchloride Polyvinyl chloride is a flame retardant material with an exceptional chemical resistance and also with lower stress cracking. PVC-U shows high mechanical strength, tensile strength and the continuou.. |
|||
Dielectric Strength | 0.984 - 40.0 kV/mm | 25.0 - 1020 kV/in | Average value: 15.1 kV/mm Grade Count:41 |
Overview of materials for Epoxy, Molded, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values.. |
|||
Dielectric Strength | 17.7 - 40.0 kV/mm | 450 - 1020 kV/in | Average value: 25.9 kV/mm Grade Count:24 |
Overview of materials for Acetal Copolymer, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values.. |