Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dielectric Strength = 28.0 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 17.3 - 28.0 kV/mm
439 - 711 kV/in
Average value: 24.9 kV/mm Grade Count:7
Overview of materials for Polycarbonate/PET Polyester Blend
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values..
Dielectric Strength 24.0 - 28.0 kV/mm
610 - 711 kV/in
AlphaGary Evoprene™ G 3290 SEBS Thermoplastic Elastomer
Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi..
Dielectric Strength 24.0 - 28.0 kV/mm
610 - 711 kV/in
AlphaGary Evoprene™ G 927 SEBS Thermoplastic Elastomer
Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi..
Dielectric Strength 24.0 - 28.0 kV/mm
610 - 711 kV/in
AlphaGary Evoprene™ G 958 SEBS Thermoplastic Elastomer
Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi..
Dielectric Strength 24.0 - 28.0 kV/mm
610 - 711 kV/in
AlphaGary Evoprene™ G 964 SEBS Thermoplastic Elastomer
Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi..
Dielectric Strength 24.0 - 28.0 kV/mm
610 - 711 kV/in
AlphaGary Evoprene™ G 966 SEBS Thermoplastic Elastomer
Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi..
Dielectric Strength 24.0 - 28.0 kV/mm
610 - 711 kV/in
AlphaGary Evoprene™ G 975 SEBS Thermoplastic Elastomer
Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi..
Dielectric Strength 24.0 - 28.0 kV/mm
610 - 711 kV/in
AlphaGary Evoprene™ G 991 SEBS Thermoplastic Elastomer
Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi..
Dielectric Strength 24.0 - 28.0 kV/mm
610 - 711 kV/in
AlphaGary Evoprene™ G 992 SEBS Thermoplastic Elastomer
Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi..
Copyright © lookpolymers.com All Rights Reserved