Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 7.90 - 15.0 kV/mm | 201 - 381 kV/in | Average value: 12.3 kV/mm Grade Count:19 |
Overview of materials for Phenolic, Novolac, Impact Grade, Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Impact Grade, Filled". Each property range of values reported is minimum and maximum .. |