Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 7.90 - 15.0 kV/mm | 201 - 381 kV/in | Average value: 12.3 kV/mm Grade Count:19 |
Overview of materials for Phenolic, Novolac, Impact Grade, Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Impact Grade, Filled". Each property range of values reported is minimum and maximum .. |
|||
Dielectric Strength | 7.90 - 16.2 kV/mm | 201 - 411 kV/in | Average value: 11.1 kV/mm Grade Count:7 |
Overview of materials for Phenolic, Novolac, Flock Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Flock Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Dielectric Strength | 7.90 - 36.0 kV/mm | 201 - 914 kV/in | Average value: 16.0 kV/mm Grade Count:55 |
Overview of materials for Phenolic, Novolac, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Glass Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Dielectric Strength | 7.90 kV/mm | 201 kV/in | Step by step; ASTM D149 |
Sumitomo Bakelite Durez® 22257 Phenolic, Injection Grade Durez 22257 Black Phenolic is a two-stage, asbestos-free, medium impact molding material. It is designed for appliance and electrical applications where additional mechanical strength is required. .. |
|||
Dielectric Strength | 7.90 kV/mm | 201 kV/in | Short Time; ASTM D149 |
Plenco 4309 Phenolic, Nodular, Injection Molded PLENCO 04309 is a heat resistant, glass reinforced phenolic molding compound offering improved mechanical strength and electrical strength properties. UL recognized under component file E40654. 0430.. |
|||
Dielectric Strength | 7.90 kV/mm | 201 kV/in | Short Time; ASTM D149 |
Plenco 7476 Phenolic, Granular, Transfer Molded PLENCO 07476 is a cotton flock filled resole phenolic molding compound, with improved physical strength, crack resistance, and is resistant to soap and detergent solutions at elevated temperatures. .. |
|||
Dielectric Strength | 7.90 kV/mm | 201 kV/in | 60 Hz, wet, SS; ASTM D149 |
Sumitomo Bakelite North America FM 3000 Cellulose Reinforced Phenolic Novolac FM 3000 is a self-lubricated cellulose reinforced phenolic molding compound, modified for applications requiring reduced friction and low wear. Information supplied by Sumitomo Bak North America... |