Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dielectric Strength = 15.0 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 7.90 - 15.0 kV/mm
201 - 381 kV/in
Average value: 12.3 kV/mm Grade Count:19
Overview of materials for Phenolic, Novolac, Impact Grade, Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Impact Grade, Filled". Each property range of values reported is minimum and maximum ..
Dielectric Strength 13.8 - 15.0 kV/mm
350 - 380 kV/in
Short Time
Bulk Molding Compounds BMC 5209 Mineral Filled, Glass Reinforced Polyester
BMC 5209 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in ex..
Dielectric Strength 13.4 - 15.0 kV/mm
340 - 380 kV/in
Short Time
Bulk Molding Compounds BMC 6241 Glass Fiber Reinforced Compound
BMC 6241 is a glass fiber-reinforced material formulated specifically for molding of industrial lighting reflectors where adequate strength is required along with a high reflectivity. It is availabl..
Dielectric Strength 13.4 - 15.0 kV/mm
340 - 380 kV/in
short time
Bulk Molding Compounds BMC 6241 Glass Reinforced BMC
BMC 6241 is a glass fiber-reinforced material formulated specifically for molding of industrial lighting reflectors where adequate strength is required along with a high reflectivity. It is availab..
Dielectric Strength 13.8 - 15.0 kV/mm
350 - 380 kV/in
Short Time
Bulk Molding Compounds BMC 5338 Mineral Filled, Glass Reinforced Polyester
BMC 5338 molding compound is a mineral Filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in ex..
Dielectric Strength 13.8 - 15.0 kV/mm
350 - 380 kV/in
short time
Bulk Molding Compounds BMC T12-15526 General Purpose Molding Compound
BMC T12-15526 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. ..
Dielectric Strength 13.8 - 15.0 kV/mm
350 - 380 kV/in
short time
Bulk Molding Compounds BMC T12-15541 General Purpose Molding Compound
BMC T12 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. Typica..