Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 15.7 - 30.2 kV/mm | 399 - 767 kV/in | Average value: 26.3 kV/mm Grade Count:19 |
Overview of materials for Polybutylene Terephthalate (PBT), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Extrusion Grade". Each property range of values reported is minimum an.. |
|||
Dielectric Strength | 15.7 kV/mm @Thickness 3.17 mm |
399 kV/in @Thickness 0.125 in |
short term; ASTM D149 |
Ensinger ENSITEP® PBT Polybutylene Terephthalate - Extruded Products
(discontinued **) ENSITEP BT is an unreinforced thermoplastic polyester derived from polybutylene terephthalate. Its excellent wear and impact resistance, low coefficient of friction, high flexural modulus, and supe.. |
|||
Dielectric Strength | 15.7 kV/mm | 399 kV/in | Short Time, 500V/sec; ASTM D149 |
Eastman 7352 PET
(discontinued **) VORIDIAN PET thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. VORIDIAN PET polyester 73.. |
|||
Dielectric Strength | 15.7 - 27.0 kV/mm | 399 - 686 kV/in | Average value: 20.4 kV/mm Grade Count:44 |
Overview of materials for Silicone, RTV, Encapsulation Grade This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Encapsulation Grade". Each property range of values reported is minimum and maximum value.. |
|||
Dielectric Strength | 15.7 kV/mm | 399 kV/in | ASTM D149 |
Plenco 504 Black (COM) Heat Resistant Mineral/Cellulose Filled Phenolic Molding Compound
(discontinued **)< Plaslok 504 is a two-stage, mineral and cellulose-filled phenolic molding compound having better impact and heat resistance than general purpose molding compounds. Since it also has good electrical.. |
|||
Dielectric Strength | 15.7 kV/mm | 399 kV/in | ASTM D149 |
Plenco 504 Black (INJ) Heat Resistant Mineral/Cellulose Filled Phenolic Molding Compound
(discontinued **)< Plaslok 504 is a two-stage, mineral and cellulose-filled phenolic molding compound having better impact and heat resistance than general purpose molding compounds. Since it also has good electrical.. |
|||
Dielectric Strength | 15.7 kV/mm @Thickness 2.00 mm |
399 kV/in @Thickness 0.0787 in |
ASTM D149 |
Manifattura Cattaneo RULON® LR Polytetrafluoroethylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Dielectric Strength | 15.7 kV/mm @Thickness 1.90 mm |
399 kV/in @Thickness 0.0748 in |
|
Momentive Performance Materials RTV12 Clear General Purpose Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Dielectric Strength | 15.7 kV/mm | 399 kV/in | 2.54 mm gap |
Solvay Specialty Polymers Galden® D02 PFPE Fluid Galden® D grades are specifically recommended for electronic reliability testing, including thermal shock and hermetic seal testing.Galden® PFPE is a line of high-performance, inert, fluorinat.. |
|||
Dielectric Strength | 15.7 kV/mm | 399 kV/in | 2.54 mm gap |
Solvay Specialty Polymers Galden® D02TS PFPE Fluid Galden® D grades are specifically recommended for electronic reliability testing, including thermal shock and hermetic seal testing.Galden® PFPE is a line of high-performance, inert, fluorinat.. |
|||
Dielectric Strength | 15.7 kV/mm | 399 kV/in | 2.54 mm gap |
Solvay Specialty Polymers Galden® D03 PFPE Fluid Galden® D grades are specifically recommended for electronic reliability testing, including thermal shock and hermetic seal testing.Galden® PFPE is a line of high-performance, inert, fluorinat.. |
|||
Dielectric Strength | 15.7 kV/mm | 399 kV/in | 2.54 mm gap |
Solvay Specialty Polymers Galden® D05 PFPE Fluid Galden® D grades are specifically recommended for electronic reliability testing, including thermal shock and hermetic seal testing.Galden® PFPE is a line of high-performance, inert, fluorinat.. |
|||
Dielectric Strength | 15.7 kV/mm | 399 kV/in | 2.54 mm gap |
Solvay Specialty Polymers Galden® DET PFPE Fluid Galden® D grades are specifically recommended for electronic reliability testing, including thermal shock and hermetic seal testing.Galden® PFPE is a line of high-performance, inert, fluorinat.. |
|||
Dielectric Strength | 15.7 kV/mm | 399 kV/in | 2.54 mm gap |
Solvay Specialty Polymers Galden® HS260 PFPE VPS Fluid Galden® LS and HS grades are specifically recommended for vapor phase soldering.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of servic.. |
|||
Dielectric Strength | 15.7 kV/mm | 399 kV/in | 2.54 mm gap |
Solvay Specialty Polymers Galden® HT170 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service.. |
|||
Dielectric Strength | 15.7 kV/mm | 399 kV/in | 2.54 mm gap |
Solvay Specialty Polymers Galden® HT200 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service.. |
|||
Dielectric Strength | 15.7 kV/mm | 399 kV/in | 2.54 mm gap |
Solvay Specialty Polymers Galden® HT230 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service.. |
|||
Dielectric Strength | 15.7 kV/mm | 399 kV/in | 2.54 mm gap |
Solvay Specialty Polymers Galden® HT55 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service.. |
|||
Dielectric Strength | 15.7 kV/mm | 399 kV/in | 2.54 mm gap |
Solvay Specialty Polymers Galden® HT80 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service.. |
|||
Dielectric Strength | 15.7 kV/mm | 399 kV/in | 2.54 mm gap |
Solvay Specialty Polymers Galden® LLS215 PFPE VPS Fluid Galden® LS and HS grades are specifically recommended for vapor phase soldering.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of servic.. |
|||
Dielectric Strength | 15.7 kV/mm | 399 kV/in | 2.54 mm gap |
Solvay Specialty Polymers Galden® LS200 PFPE VPS Fluid Galden® LS and HS grades are specifically recommended for vapor phase soldering.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of servic.. |
|||
Dielectric Strength | 15.7 kV/mm | 399 kV/in | Short Time; ASTM D149 |
Sumitomo Bakelite Durez® 118 Phenolic, Compression Grade Durez 118 Black Phenolic is a two-stage, asbestos free, general purpose molding material. It exhibits improved impact strength and resistance to flexural fatigue for demanding automotive, electrica.. |
|||
Dielectric Strength | 15.7 kV/mm | 399 kV/in | ASTM D149 |
Styron CALIBREâ„¢ 2060-6 Polycarbonate CALIBREâ„¢ 2060-6 resin is designed for medical applications which use steam or ethylene oxide for sterilization. This material has excellent retention of physical properties and optical clarity.. |
|||
Dielectric Strength | 15.7 kV/mm | 399 kV/in | ASTM D149 |
Styron CALIBREâ„¢ 2061-6 Polycarbonate CALIBREâ„¢ 2061-6 resin is used in applications involving steam or ethylene oxide for sterilization - though suitability for use in these applications is dependent upon autoclave cycle times and .. |
|||
Dielectric Strength | 15.7 kV/mm | 399 kV/in | Step by step; ASTM D149 |
Sumitomo Bakelite Durez® 32633 Glass Filled Phenolic, Injection Grade Durez 32633 Black Phenolic is a two-stage, glass filled, special purpose molding compound. It is designed for applications requiring high physical strengths, dimensional stability, and heat resista.. |
|||
Dielectric Strength | 15.7 kV/mm | 399 kV/in | Step by step; ASTM D149 |
Sumitomo Bakelite Sumikon® PM-9640 Glass Filled Phenolic Two stage glass fiber filled black phenolic. It is especially designed for applications requiring high strength and dimensional stability with excellent heat resistance. PM-9640 is widely used in .. |
|||
Dielectric Strength | 15.7 kV/mm | 399 kV/in | Short Time, 500V/sec; ASTM D149 |
Eastman Eastar EN052 Polyester Eastar Polyester EN052 is a thermoplastic condensation homopolymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. It has been crystalliz.. |
|||
Dielectric Strength | 15.7 kV/mm | 399 kV/in | Short Time, 500V/sec; ASTM D149 |
Eastman Eastar MN052 Polyester, Natural Eastar polyester MN052 is a thermoplastic condensation homopolymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. It has been crystalliz.. |
|||
Dielectric Strength | 15.7 kV/mm | 399 kV/in | ASTM D149 |
Plaslok 504 Black (INJ) Heat Resistant Mineral/Cellulose Filled Phenolic Molding Compound
(discontinued **)&l Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 504 is a two-stage, mineral and cellu.. |
|||
Dielectric Strength | 15.7 kV/mm | 399 kV/in | 2.54 mm gap |
Solvay Specialty Polymers Galden® HT110 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service tem.. |