Electrical Properties Metric English Comments
Dielectric Strength 15.0 - 42.9 kV/mm
381 - 1090 kV/in
Average value: 22.3 kV/mm Grade Count:104
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an..