Electrical Properties Metric English Comments
Dielectric Strength 15.0 - 42.9 kV/mm
381 - 1090 kV/in
Average value: 22.3 kV/mm Grade Count:104
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an..
Dielectric Strength 17.7 - 43.0 kV/mm
450 - 1090 kV/in
Average value: 27.4 kV/mm Grade Count:22
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar..
Dielectric Strength 19.0 - 43.0 kV/mm
483 - 1090 kV/in
Average value: 25.5 kV/mm Grade Count:8
Overview of materials for Acetal Copolymer, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values ..
Dielectric Strength 19.7 - 43.0 kV/mm
500 - 1090 kV/in
Average value: 31.2 kV/mm Grade Count:24
Overview of materials for Nylon 6, Glass Filled, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu..
Dielectric Strength 17.7 - 43.0 kV/mm
450 - 1090 kV/in
Average value: 28.8 kV/mm Grade Count:50
Overview of materials for Polypropylene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of..
Dielectric Strength 19.7 - 43.0 kV/mm
500 - 1090 kV/in
Average value: 33.0 kV/mm Grade Count:13
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40%
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. ..
Dielectric Strength 24.0 - 43.0 kV/mm
610 - 1090 kV/in
Average value: 41.1 kV/mm Grade Count:11
Overview of materials for Polypropylene, Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values..