Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 17.3 kV/mm | 440 kV/in | |
Resinlab® EP1121 Clear Electronic Grade Epoxy Encapsulant Resinlab™ EP1121 Clear is a two part unfilled electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexible polymer. I.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | |
Resinlab® EP1325 Thixotropic, Heat Curing Epoxy Adhesive Resinlab™ EP1325 and EP1325LV are one part thixotropic, heat curing epoxy adhesives. They can also be used as a small mass potting compounds, staking or damming adhesives, or polymer systems where .. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | |
Resinlab® EP1330 Heat Cure Epoxy Polymer System Resinlab™ EP1330 and EP1330LV are one part heat cure epoxy polymer systems. They can also be used as a small mass potting or staking compounds, or a dam adhesive in and “dam and fill” application.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Elastoblend® PA6/6 GF30 IM HS L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Elastoblend® PA6/6 GF30 IM2 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Elastoblend® PA6/6 GF43 IM L 43% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 43% Filler by WeightAdditive: Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedTPCI# 6439.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Elastoblend® PA6/6 HI BK Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedUl File Number: E157318Appearance: BlackProce.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Elastoblend® PA6/6 IM L W Nylon 66 Availability: North AmericaForms: PelletsAdditive: Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc... |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill FR® PA6/6 GF25 FR BK 25% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and LubricatedAppear.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6/6 GF33 BK024 33% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: LubricantFeatures: Lubricated Appearance: BlackInformation provided by TP Comp.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6/6 GF33 NAT001 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightUL File Number: E157318Appearance: Black and Natural ColorTPCI# 9475101Information provi.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Luriblend® PA6/6 GF10 TL10 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: Heat Stabilizer and PTFE Lubricant(5%)Features: Lubricated, Good Wear Resistance, Low Fricti.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Luriblend® TPX-PA6-03034 Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber ReinforcementAdditive: LubricantFeatures: Lubricated, Good Wear Resistance and Low FrictionAppearance: BlackInformation pro.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Plastiblend® PA6/6 GF40 IM HS L BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Plastiblend® PA6/6,6 IM HS L Nylon 6/66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Copolymer, Impact Modified and LubricatedProcessing Method: Injection Mold.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Elastoblend® PA6/6 GF30 IM2 HS BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Elastoblend® PA6/6 GF30 IM2 UV 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: UV Stabilizer, Heat Stabilizer, Lubricant and Impact ModifierFeatures: Good UV.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Elastoblend® PA6/6 GF33 IM HS L BKN 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Elastoblend® PA6/6 IM 408 HS L Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformati.. |
|||
Dielectric Strength | >= 17.3 kV/mm @Thickness 3.17 mm |
>= 440 kV/in @Thickness 0.125 in |
|
Master Bond EP112 Low Viscosity Heat Curing Cycloaliphatic Epoxy Adhesive Master Bond Polymer System EP112 is a solventless, low viscosity two component cycloaliphatic epoxy resin system which is specifically designed for high performance outdoor and indoor electrical & e.. |
|||
Dielectric Strength | 17.3 kV/mm @Thickness 3.17 mm |
440 kV/in @Thickness 0.125 in |
|
Master Bond EP30HV Optically Clear, High Strength Two Part Epoxy Description: Master Bond EP30HV is a lower viscosity, two component epoxy system for high performance bonding, sealing, coating and potting. It is formulated to cure at room temperature or more rapi.. |
|||
Dielectric Strength | 17.3 kV/mm @Thickness 3.17 mm |
440 kV/in @Thickness 0.125 in |
|
Master Bond EP41S-1HTND Non-Drip, High Performance Epoxy Adhesive Description: Master Bond EP41S-1HTND is a two component epoxy resin system for high performance bonding, sealing and coating. It has a 100 to 30 mix ratio by weight and its viscosity is a smooth pas.. |
|||
Dielectric Strength | 17.3 kV/mm @Thickness 3.17 mm |
440 kV/in @Thickness 0.125 in |
|
Master Bond EP36AN One Part, Toughened, B-Stage Epoxy Description: Master Bond EP36AN is a unique one component, high performance epoxy for bonding, encapsulation, potting and coating featuring thermal conductivity, electrical insulation and high tempe.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | |
Dow Corning 3-4241 DIELECTRIC TOUGH GEL KIT Two-part, translucent green, RT or heat cure, UV indicator, long working time, tough primerless chemical adhesion, UL 94 V-1 flammability classification.Information provided by Dow Corning |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | ASTM D149 |
Arlon LW401Y##-M1 0.040" (1.02 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 1 inch wide, 40 mil thick, Yellow, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll lengt.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | |
Aremco Aremco-Bond™ 631 High Performance Epoxide Clear-Amber, 1:1, Good Bond Strength and Corrosion Resistance.Also available filled with aluminum oxide (Alumina) or pigments. |
|||
Dielectric Strength | >= 17.3 kV/mm | >= 440 kV/in | |
Arlon 44250R011 0.011" (0.279 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data represents typical values for the production material. The data should not be used to wri.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | |
Resinlab® EP1195 Flame Retardant Epoxy Casting Resin Resinlab™ EP1195 is a low viscosity, fast gelling, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File # E1.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | |
Resinlab® UR3005 Clear Two Part Urethane Elastomer Resinlab™ UR 3005 Clear is a two component, room temperature curing polybutadiene polyurethane casting and potting system. It is designed to cure completely at room temperature. UR 3005 Clear provi.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill FR® PA6/6 GF25 FR 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightUL File Number: E157318TPCI# 9085101Information provided by TP Composites, Inc. |