Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Resinlab® UR3005 Clear Two Part Urethane Elastomer

Category Polymer , Adhesive , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Adhesive , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer Resinlab®
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Resinlab® UR3005 Clear Two Part Urethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Resinlab™ UR 3005 Clear is a two component, room temperature curing polybutadiene polyurethane casting and potting system. It is designed to cure completely at room temperature. UR 3005 Clear provides excellent environmental protection while having tenacious adhesion to various metals, plastics and other common assembly materials. UR 3005 Clear is an unfilled system that has a high degree of flexibility at temperatures as low as –40°C and provides for low stress on sensitive SMT components. It provides excellent moisture resistance and can withstand 125°C continuous operation. It also has a low viscosity, which facilitates flow and penetration into difficult areas. It is well suited to automated meter mix operations. UR 3005 Clear is a DOT non-hazardous material and contains no TDI, MOCA, or other reportable substances. Both components are moderately moisture sensitive and must be kept away from atmospheric moisture during storage. After opening a sealed container, thoroughly purge the remaining air space with dry inert gas such as nitrogen (or equivalent) before closing the container.Information Provided by Resinlab L.L.C., an Ellsworth Adhesives Company.
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
Part B
0.960 g/cc
0.960 g/cc
Mixed
1.11 g/cc
1.11 g/cc
Part A
Viscosity 200 cP
200 cP
Part A (Isocyanate)
4000 cP
4000 cP
Mixed
7000 cP
7000 cP
Part B (Polyol)
Mechanical Properties Metric English Comments
Hardness, Shore A 55

@Temperature 25.0 °C
55

@Temperature 77.0 °F
75

@Temperature -40.0 °C
75

@Temperature -40.0 °F
Tensile Strength, Yield 1.03 MPa
150 psi
Elongation at Break 150 %
150 %
Thermal Properties Metric English Comments
CTE, linear 120 µm/m-°C
66.7 µin/in-°F
Thermal Conductivity 0.140 W/m-K
0.972 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 125 °C
257 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Electrical Properties Metric English Comments
Volume Resistivity 8.00e+12 ohm-cm
8.00e+12 ohm-cm
Dielectric Constant 3.2

@Frequency 100 Hz,
Temperature 25.0 °C
3.2

@Frequency 100 Hz,
Temperature 77.0 °F
Dielectric Strength 17.3 kV/mm
440 kV/in
Processing Properties Metric English Comments
Pot Life 10 - 20 min
10 - 20 min
Mass: 100g
Descriptive Properties Value Comments
Color Clear
Demold Time (hours) 4-8
Mix Ratio 1:6
Volume
100:510
Weight