Electrical Properties Metric English Comments
Dielectric Strength 49.0 kV/mm

@Thickness 3.20 mm
1240 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics NORYL PX9406K PPE+HIPS (Asia Pacific)
NORYL* PX9406K resin may be suitable for consumer electronics applications. Flame retardant used is non-halogenated. UL94 V0 at 1.5 mm, 5VB at 2 mm, and 5VA at 2.5 mm. RTI (impact) = 105 C
Dielectric Strength 49.0 kV/mm

@Thickness 3.20 mm
1240 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
SABIC Innovative Plastics NORYL NH5020 PPE+PS
Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta..
Dielectric Strength 49.0 kV/mm

@Thickness 3.20 mm
1240 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
SABIC Innovative Plastics NORYL NH5020 PPE+PS (Asia Pacific)
Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta..
Dielectric Strength 49.0 kV/mm

@Thickness 3.20 mm
1240 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
SABIC Innovative Plastics NORYL NH5020 PPE+PS (Europe-Africa-Middle East)
Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta..
Dielectric Strength 49.0 kV/mm

@Thickness 3.20 mm
1240 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
SABIC Innovative Plastics NORYL N1250 PPE+HIPS (Asia Pacific)
Noryl* N1250 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow , this resin also uses non-chlorinated, non-brominated FR ad..
Dielectric Strength 49.0 kV/mm
1240 kV/in
ASTM D149
Westlake Plastics Zelux® 20% GF Polycarbonate 20% Glass Filled
Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and ..
Dielectric Strength 49.0 kV/mm
1240 kV/in
Full-wave Impulse; ASTM D3426
DuPont™ Nomex® 410 Paper, 30 mil Nominal Thickness
Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is ..
Dielectric Strength >= 49.0 kV/mm
>= 1240 kV/in
DIN 53481/VDE 0303
BASF Elastollan® 1164D Polyether Type Polyurethane Elastomer
Recommended for injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes. They exhi..
Dielectric Strength >= 49.0 kV/mm
>= 1240 kV/in
DIN 53481/VDE 0303
BASF Elastollan® C-64D Polyester Type Polyurethane Elastomer
Recommended for injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellent oil, fue..