Material Notes:
Arlon 45N is a tough, high Tg (175°C by DSC) multifunctional epoxy laminate and prepreg system designed for use in a variety of higher layer count MLBs. Processable using conventional FR-4 conditions. 45N is supplied to meet the requirements of IPC-4101/24High Tg by DSC (175°C)Resists barrel cracking and inner layer copper cracking during fabricationResistant to Measling and Solder shock DefectsSuitable for most lead-free applicationsRoHS/WEEE compliantTypical Applications:Automotive Under-hood applicationsBackplanes and Mother BoardsBall Grid Array PackagingHigh layer count MLBsThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Physical Properties Metric English Comments
Density 1.85 g/cc
0.0668 lb/in³
ASTM D792 Method A
Water Absorption 0.10 %
0.10 %
IPC TM-650 2.6.2.1
Mechanical Properties Metric English Comments
Modulus of Elasticity 19.3 GPa
2800 ksi
IPC TM-650 2.4.18.3
Poissons Ratio 0.20
0.20
ASTM D3039
Peel Strength 1.40 kN/m
8.00 pli
To Copper (1 oz./35 micron); After Process Solutions; IPC TM-650 2.4.8
1.40 kN/m
8.00 pli
To Copper (1 oz./35 micron); After Thermal Stress; IPC TM-650 2.4.8
1.40 kN/m
8.00 pli
To Copper (1 oz./35 micron); At Elevated Temperatures; IPC TM-650 2.4.8.2
Thermal Properties Metric English Comments
CTE, linear 14.0 - 16.0 µm/m-°C
7.78 - 8.89 µin/in-°F
IPC TM-650 2.4.41
CTE, linear, Transverse to Flow 55.0 µm/m-°C
30.6 µin/in-°F
z, below Tg; IPC TM-650 2.4.24
200 µm/m-°C
111 µin/in-°F
z, above Tg; IPC TM-650 2.4.24
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
ASTM E1461
Glass Transition Temp, Tg 175 °C
347 °F
DSC; IPC TM-650 2.4.25
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 2.60e+13 ohm-cm
2.60e+13 ohm-cm
C96/35/90; IPC TM-650 2.5.17.1
3.30e+13 ohm-cm
3.30e+13 ohm-cm
E24/125; IPC TM-650 2.5.17.1
Surface Resistance 4.00e+10 ohm
4.00e+10 ohm
C96/35/90; IPC TM-650 2.5.17.1
2.90e+13 ohm
2.90e+13 ohm
E24/125; IPC TM-650 2.5.17.1
Dielectric Constant 4.2 - 4.6

@Frequency 1.00e+6 Hz
4.2 - 4.6

@Frequency 1.00e+6 Hz
may vary with resin %; IPC TM-650 2.5.5.3
Dielectric Strength 59.1 kV/mm
1500 kV/in
IPC TM-650 2.5.6.2
Dissipation Factor 0.025

@Frequency 1.00e+6 Hz
0.025

@Frequency 1.00e+6 Hz
IPC TM-650 2.5.5.3
Arc Resistance 65 sec
65 sec
IPC TM-650 2.5.1
Descriptive Properties Value Comments
Z-Axis Expansion (%) 2.4
IPC TM-650 2.4.24 (50-260°C)