Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Amity Thermosets ATO 142 Phenolic Molding Organic Filler, Compression Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic
Manufacturer Amity Thermosets
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Amity Thermosets ATO 142 Phenolic Molding Organic Filler, Compression Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-black, brownMedium/hard flow Applications: Electric switchgear components ( eg. relays ) Telecommunication equipment partsElectronic equipment partsAutomotive ( electronic and electrical ) parts Medium tension pulleysHigh gloss toilet seatsBig meter coversCircuit breaking switchesCoffee machine basesAutomobile light and signaling switches Moulding which ought to have overall good propertiesSolenoid switch covers, knobs and tops (superior quality), etc. Information provided by Amity Thermosets Limited
Physical Properties Metric English Comments
Density 1.35 - 1.38 g/cc
0.0488 - 0.0499 lb/in³
Molding; IS 867-1963
Apparent Bulk Density 0.620 - 0.680 g/cc
0.0224 - 0.0246 lb/in³
IS 867-1963
Water Absorption 0.30 - 0.40 %
0.30 - 0.40 %
IS 13411-1993
Linear Mold Shrinkage 0.0075 - 0.0083 cm/cm
0.0075 - 0.0083 in/in
IS 13411-1992
Mechanical Properties Metric English Comments
Tensile Strength at Break 50.0 - 60.0 MPa
7250 - 8700 psi
5 mm/min.; IS 867-1963
Shear Strength 70.0 - 84.0 MPa
10200 - 12200 psi
IS 867-1963
Izod Impact, Notched 0.250 - 0.400 J/cm
0.468 - 0.749 ft-lb/in
IS 13411-1992
Electrical Properties Metric English Comments
Volume Resistivity 3.16e+10 - 3.16e+11 ohm-cm
3.16e+10 - 3.16e+11 ohm-cm
IS 3396-1979
Surface Resistance 1.00e+10 - 1.00e+11 ohm
1.00e+10 - 1.00e+11 ohm
IS 3396-1979
Dielectric Strength 5.50 - 7.50 kV/mm

@Temperature 90.0 °C
140 - 191 kV/in

@Temperature 194 °F
IS 2584-1963
Comparative Tracking Index >= 125 V
>= 125 V
2824-1975
Processing Properties Metric English Comments
Mold Temperature 160 - 180 °C
320 - 356 °F
Injection Pressure 15.68 - 34.3 MPa
2274 - 4970 psi
Mold Pressure
Cure Time 0.333 - 0.417 min
0.00556 - 0.00694 hour
per mm
Shelf Life 12.0 Month
12.0 Month
10-25°C