Polymer Property : Dielectric Strength = 914 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 7.90 - 36.0 kV/mm
201 - 914 kV/in
Average value: 16.0 kV/mm Grade Count:55
Overview of materials for Phenolic, Novolac, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Glass Filled". Each property range of values reported is minimum and maximum values o..
Dielectric Strength 18.0 - 36.0 kV/mm
457 - 914 kV/in
Average value: 22.7 kV/mm Grade Count:29
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are..