Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.20e+12 ohm-cm | 1.20e+12 ohm-cm | ASTM D247 |
Plenco 2408 Phenolic, Granular, Compression Molded PLENCO 02408 is a general purpose, organic filled phenolic molding compound, offering excellent cosmetic characteristics and improved electrical strength properties. UL recognized under component fi.. |
|||
Volume Resistivity | 1.20e+12 ohm-cm | 1.20e+12 ohm-cm | ASTM D247 |
Plenco 6527 Phenolic, Granular, Transfer Molded PLENCO 06527 is a woodflour and mineral filled resole phenolic molding compound.Information supplied by Plenco. |
|||
Volume Resistivity | 1.20e+12 ohm-cm | 1.20e+12 ohm-cm | ASTM D247 |
Plenco 6990 Phenolic, Briquette, Transfer Molded PLENCO 06990 is a glass and mineral filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco. |
|||
Volume Resistivity | 1.20e+12 ohm-cm | 1.20e+12 ohm-cm | ASTM D247 |
Plenco 2571 Phenolic, Granular, Injection Molded PLENCO 02571 is a general purpose, organic filled phenolic molding compound offering optimum cure characteristics while maintaining excellent mechanical and electrical properties. UL recognized unde.. |
|||
Volume Resistivity | 1.20e+12 ohm-cm | 1.20e+12 ohm-cm | |
Dow Corning FLUOROGEL® 4-8022 One-part, translucent, heat cure, UV indicator, fuel and solvent resistant.Information provided by Dow Corning |