Polymer Property : Volume Resistivity = 1.60e+13 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 1.60e+13 ohm-cm
1.60e+13 ohm-cm
ASTM D257
Proto3000 Duraform® AF Selective Laser Sintering (SLS®) Prototyping Polymer
Description: Polyamide (nylon) material with metallic appearance for real-world physical testing and functional use.Features:Metallic appearance with nice surface finishGood powder recycle character..
Volume Resistivity 1.60e+13 ohm-cm
1.60e+13 ohm-cm
ASTM D247
Plenco 7507 Phenolic, Granular, Compression Molded
PLENCO 07507 is an organic reinforced phenolic molding compound offering improved dimensional stability under humid conditions. 07507 offers excellent resistance to degradation from detergent solut..
Volume Resistivity >= 1.60e+13 ohm-cm
>= 1.60e+13 ohm-cm
Epoxy Technology EPO-TEK® 353ND Black High Temperature Epoxy
Product Description: EPO TEK® 353ND Black is a a two component, high temperature epoxy designed for semiconductor, hybrid, fiber optic, and medical applicationsAdvantages & Application Notes: EPO T..
Volume Resistivity 1.60e+13 ohm-cm
1.60e+13 ohm-cm
ASTM D257
3D Systems DuraForm® AF Nylon for SLS® Systems
Polyamide (nylon) material with metallic appearance for real-world physical testing and functional use. For use with all selective laser sintering SLS® systems.ApplicationsHousings and enclosuresCo..
Volume Resistivity 1.60e+13 ohm-cm
1.60e+13 ohm-cm
ASTM D257
ALM PA 605-A Filled Nylon 12 Prototyping Polymer
50% Aluminum filled nylon 12 that can produce accurate parts with excellent part strength and surface detail.Drop in replacement for other commercially available 50% aluminum filled materials with a..