Polyamide (nylon) material with metallic appearance for real-world physical testing and functional use. For use with all selective laser sintering SLS® systems.ApplicationsHousings and enclosuresConsumer productsAppropriate for low- to mid-volume rapid manufacturingParts requiring machining or joining with adhesivesComplex production and prototype plastic partsForm, fit or functional prototypesParts requiring stiffnessThermally stressed partsPlastic parts requiring a metallic appearanceAll information provided by 3D Systems.
Physical Properties Metric English Comments
Bulk Density 0.890 g/cc

@Temperature 25.0 °C
0.0322 lb/in³

@Temperature 77.0 °F
tap
Density 0.690 g/cc

@Temperature 25.0 °C
0.0249 lb/in³

@Temperature 77.0 °F
bulk
Mechanical Properties Metric English Comments
Hardness, Shore D 75
75
ASTM D2240
Tensile Strength, Ultimate 35.0 MPa
5080 psi
ASTM D638
Elongation at Break 1.5 %
1.5 %
ASTM D638
Tensile Modulus 3.96 GPa
574 ksi
ASTM D638
Flexural Strength 44.0 MPa
6380 psi
ASTM D790
Flexural Modulus 3.517 GPa
510.1 ksi
ASTM D790
Izod Impact, Notched 0.587 J/cm

@Temperature 23.0 °C
1.10 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched 1.23 J/cm

@Temperature 23.0 °C
2.30 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 109 µm/m-°C

@Temperature 35.0 - 172 °C
60.6 µin/in-°F

@Temperature 95.0 - 342 °F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 180 °C
356 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 137 °C
279 °F
ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.60e+13 ohm-cm
1.60e+13 ohm-cm
ASTM D257
Surface Resistance 6.00e+12 ohm
6.00e+12 ohm
ASTM D257
Dielectric Constant 14.5

@Frequency 1000 Hz
14.5

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 1.80 kV/mm
45.7 kV/in
ASTM D149
Descriptive Properties Value Comments
Appearance Light grey metallic
Users viewing this material also viewed the following: