Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.90e+11 ohm-cm | 1.90e+11 ohm-cm | ASTM D247 |
Plenco 4349 Phenolic, Granular, Transfer Molded PLENCO 04349 is a heat resistant, mineral filled phenolic molding compound offering optimized cure characteristics, and excellent heat resistant properties. PLENCO 04349 is also formulated to offer .. |
|||
Volume Resistivity | 1.90e+11 ohm-cm | 1.90e+11 ohm-cm | ASTM D247 |
Plenco 4485 Phenolic, Granular, Injection Molded PLENCO 04485 is a mineral filled phenolic molding compound offering excellent heat resistance, electrical resistance, and dimensional stability. UL recognized under component file E40654. 04485 is a.. |
|||
Volume Resistivity | 1.90e+11 ohm-cm | 1.90e+11 ohm-cm | ASTM D247 |
Plenco 6015 Phenolic, Briquette, Injection Molded PLENCO 06015 is a glass and mineral filled phenolic molding compound offering improved mechanical strength, dimensional stability and excellent electrical properties. 06015 is available in black.Inf.. |