Electrical Properties Metric English Comments
Volume Resistivity 1.90e+11 ohm-cm
1.90e+11 ohm-cm
ASTM D247
Plenco 4349 Phenolic, Granular, Transfer Molded
PLENCO 04349 is a heat resistant, mineral filled phenolic molding compound offering optimized cure characteristics, and excellent heat resistant properties. PLENCO 04349 is also formulated to offer ..
Volume Resistivity 1.90e+11 ohm-cm
1.90e+11 ohm-cm
ASTM D247
Plenco 4485 Phenolic, Granular, Injection Molded
PLENCO 04485 is a mineral filled phenolic molding compound offering excellent heat resistance, electrical resistance, and dimensional stability. UL recognized under component file E40654. 04485 is a..
Volume Resistivity 1.90e+11 ohm-cm
1.90e+11 ohm-cm
ASTM D247
Plenco 6015 Phenolic, Briquette, Injection Molded
PLENCO 06015 is a glass and mineral filled phenolic molding compound offering improved mechanical strength, dimensional stability and excellent electrical properties. 06015 is available in black.Inf..