Plenco 4349 Phenolic, Granular, Transfer Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Mineral Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 4349 Phenolic, Granular, Transfer Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 04349 is a heat resistant, mineral filled phenolic molding compound offering optimized cure characteristics, and excellent heat resistant properties. PLENCO 04349 is also formulated to offer exceptional cosmetic characteristics in the molded product. UL recognized under component file E40654. 04349 is available in black.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.640 g/cc
0.0231 lb/in³
ASTM D1895
Density 1.56 g/cc
0.0564 lb/in³
ASTM D792
Water Absorption 0.118 %
0.118 %
ASTM D570
Linear Mold Shrinkage 0.0043 cm/cm
0.0043 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 91
91
ASTM D785
Tensile Strength, Ultimate 51.0 MPa
7400 psi
ASTM D638
Elongation at Break 0.71 %
0.71 %
ASTM D638
Tensile Modulus 9.40 GPa
1360 ksi
ASTM D638
Flexural Strength 77.0 MPa
11200 psi
ASTM D790
Flexural Modulus 9.10 GPa
1320 ksi
ASTM D790
Compressive Strength 197 MPa
28600 psi
ASTM D695
Izod Impact, Notched 0.155 J/cm
0.290 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.188 J/cm²
0.895 ft-lb/in²
ASTM D256
Impact 97
97
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 38.0 µm/m-°C

@Temperature 40.0 - 130 °C
21.1 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Maximum Service Temperature, Air 213 °C
415 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 211 °C
412 °F
ASTM D648
Flammability, UL94 V-1

@Thickness 1.50 mm
V-1

@Thickness 0.0591 in
Shrinkage 0.173 %
0.173 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 1.90e+11 ohm-cm
1.90e+11 ohm-cm
ASTM D247
Dielectric Constant 5.8
5.8
ASTM D150
Dielectric Strength 11.1 kV/mm
282 kV/in
Short Time; ASTM D149
Dissipation Factor 0.063
0.063
ASTM D150
Arc Resistance 170 sec
170 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638
Users viewing this material also viewed the following: