Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 3.2e+11 - 1.0e+12 ohm-cm | 3.2e+11 - 1.0e+12 ohm-cm | IS 3396-1979 |
Amity Thermosets ATF 197 Phenolic Molding Inorganic and glass Filler, Compression Molded Characteristics:Flame retardantSpark resistant Good electrical insulationHeat stability ( 200°C )Good mouldability Low water absorptionLow shrinkageColor-blackSoft/medium flow Applications:Switchg.. |
|||
Volume Resistivity | 3.2e+11 - 3.2e+12 ohm-cm | 3.2e+11 - 3.2e+12 ohm-cm | IS 3396-1979 |
Amity Thermosets ATI 101 Phenolic Molding Organic Filler, Injection Molded Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-blackVery soft flow Applications: Electric swit.. |
|||
Volume Resistivity | 3.2e+11 - 3.2e+12 ohm-cm | 3.2e+11 - 3.2e+12 ohm-cm | IS 3396-1979 |
Amity Thermosets ATO 156 Phenolic Molding Glass Filler, Compression Molded Characteristics:High electrical insulationHigh mechanical strengthDimensional stabilityLow water absorptionColor-black Medium flow Applications: High electric insulation componentsHigh voltage swit.. |
|||
Volume Resistivity | 3.2e+11 - 1.0e+12 ohm-cm | 3.2e+11 - 1.0e+12 ohm-cm | IS 3396-1979 |
Amity Thermosets ATS 1612 Phenolic Molding Nylon, inorganic, and glass Filler, Compression Molded Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackSoft/Medium flow Applications:R.. |
|||
Volume Resistivity | 3.2e+11 - 1.0e+12 ohm-cm | 3.2e+11 - 1.0e+12 ohm-cm | IS 3396-1979 |
Amity Thermosets ATS 751 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded Characteristics:High impact strength Dimensional stabilityHigh mechanical strengthHeat stability ( 200°C )Good media resistance ( eg. Oil, water ) Low shrinkageGood electrical resistanceColor-brown.. |
|||
Volume Resistivity | 3.2e+11 - 1.0e+12 ohm-cm | 3.2e+11 - 1.0e+12 ohm-cm | IS 3396-1979 |
Amity Thermosets ATO 1510 Phenolic Molding Glass fiber Filler, Compression Molded Characteristics:Shock resistantElectrical low lossHigh mechanical strengthHeat stableHigh electrical insulationDimensional stabilityGood mechanical tension bearing strengthMedium copper adhesionColo.. |
|||
Volume Resistivity | 3.2e+11 - 3.2e+12 ohm-cm | 3.2e+11 - 3.2e+12 ohm-cm | IS 3396-1979 |
Amity Thermosets ATO 159 Phenolic Molding Glass/ inorganic Filler, Compression Molded Characteristics:High electrical insulationHigh mechanical strengthDimensional stabilityLow water absorptionColor-black Medium flow Applications: High electric insulation componentsHigh voltage swit.. |
|||
Volume Resistivity | 3.2e+11 - 1.0e+12 ohm-cm | 3.2e+11 - 1.0e+12 ohm-cm | IS 3396-1979 |
Amity Thermosets ATS 155 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded Characteristics:Shock resistantElectrical low lossHigh mechanical strengthHeat stableHigh electrical insulationDimensional stabilityGood mechanical tension bearing strengthGood copper adhesion Color.. |
|||
Volume Resistivity | 3.2e+11 - 1.0e+12 ohm-cm | 3.2e+11 - 1.0e+12 ohm-cm | IS 3396-1979 |
Amity Thermosets ATS 1613-G Phenolic Molding Nylon and inorganic Filler, Compression Molded Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackSoft/Medium flow Applications:R.. |