Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | >= 5.00e+16 ohm-cm | >= 5.00e+16 ohm-cm | ISO.167 DN.53482 |
Polimersan Plastics POLIPOLEN® (Polyethylene) HD-PE 300 PE 300: Polyethylene with high density. POLIPOLEN® PE (POLYETHYLENE) is maintained from coke oven gas or from natural gas or from Ethene or Ethane which is produced by cracking of petroleum. Monom.. |
|||
Volume Resistivity | >= 5.00e+16 ohm-cm | >= 5.00e+16 ohm-cm | ISO.167 DN.53482 |
Polimersan Plastics POLIPOLEN® (Polyethylene) HD-PE 500 PE 500: Polyethylenes with molecular weight higher than 500,000 gr/mol. POLIPOLEN® PE (POLYETHYLENE) is maintained from coke oven gas or from natural gas or from Ethene or Ethane which is produce.. |
|||
Volume Resistivity | >= 5.00e+16 ohm-cm | >= 5.00e+16 ohm-cm | ISO.167 DN.53482 |
Polimersan Plastics POLIPOLEN® (Polyethylene) UHMW-PE 1000 PE 1000: Polyethylene with very high molecular weight (UHMW - PE 1000; Ultra High Molecular Weight Polyethylene). Polyethylenes with molecular weight higher than 3 million gr/mol. POLIPOLEN® PE (P.. |
|||
Volume Resistivity | >= 5.00e+16 ohm-cm | >= 5.00e+16 ohm-cm | ISO.167 DN.53482 |
Polimersan Plastics POLIPOLEN® (Polyethylene) HD-PE 500 PE 500: Polyethylenes with molecular weight higher than 500,000 gr/mol. POLIPOLEN® PE (POLYETHYLENE) is maintained from coke oven gas or from natural gas or from Ethene or Ethane which is produce.. |
|||
Volume Resistivity | 5.00e+16 ohm-cm | 5.00e+16 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Udel® P-1710 Polysulfone (PSU)
(Unverified Data**) Udel P-1710 polysulfone (PSU) is a tough, rigid, high-strength thermoplastic that is suitable for continuous use up to 300°F (149°C). The resin is resistant to oxidation and hydrolysis and withsta.. |
|||
Volume Resistivity | 5.00e+16 ohm-cm | 5.00e+16 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Udel® P-1800 Polysulfone (PSU)
(discontinued **) Udel P-1800 is a powdered grade of polysulfone with molecular weight similar to that of Udel P-1700 polysulfone. It is well suited for the fabrication of porous membranes that can be made into hollo.. |
|||
Volume Resistivity | 5.00e+16 ohm-cm | 5.00e+16 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Udel® P-1835 Polysulfone (PSU)
(discontinued **) Udel P-1835 polysulfone is a powdered grade well suited for the fabrication of porous membranes. The membranes can be made into hollow fibers, tubes, plates, or spiral wound elements. They are used .. |
|||
Volume Resistivity | 5.00e+16 ohm-cm | 5.00e+16 ohm-cm | IEC 60093 |
Manifattura Cattaneo PVDF Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Volume Resistivity | 5.00e+16 ohm-cm | 5.00e+16 ohm-cm | ASTM D257 |
Techmer ES Elastoblend® PBT IM Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 5.00e+16 ohm-cm | 5.00e+16 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Udel® P-3703 Polysulfone (PSU) Udel® P-3703 is a high-flow grade of polysulfone intended for injection molding applications with thin walls or long flow lengths. This grade has higher flow than Udel® P-1700 and a slightly g.. |
|||
Volume Resistivity | 5.00e+16 ohm-cm | 5.00e+16 ohm-cm | ASTM D257 |
Samyang Triloy® 130 PC/PBT alloy Characteristics:Impact resistantChemical resistantDimensional stabilityProcessabilityGood flowApplications:Automotive bumperAutomotive outdoor handleAll information provided by Samyang |
|||
Volume Resistivity | 5.00e+16 ohm-cm | 5.00e+16 ohm-cm | ASTM D257 |
Samyang Triloy® 210 PC/ABS alloy Characteristics:Impact resistantHeat resistantGood flowApplications:Camera partsExterior panelCluster fasciaWheel coverStructural applicationI/P. core panelHelmet shellGlove box doorCowl vent grillA.. |
|||
Volume Resistivity | 5.00e+16 ohm-cm | 5.00e+16 ohm-cm | ASTM D257 |
Samyang Triloy® 215 PC/ABS alloy Characteristics:Dimensional stabilityHigh heat resistanceGood flowApplications:Camera partsExterior panelCluster fasciaWheel coverStructural applicationI/P. core panelHelmet shellGlove box doorCowl .. |
|||
Volume Resistivity | 5.00e+16 ohm-cm | 5.00e+16 ohm-cm | ASTM D257 |
Samyang Triloy® 220 Polymer Alloy, High Impact Excellent impact, formability and weather resistance.220 is a high impact grade.Applications: Automotive instrument panels and knob typesInformation provided by Samyang. |
|||
Volume Resistivity | 5.00e+16 ohm-cm | 5.00e+16 ohm-cm | ASTM D257 |
Samyang Triloy® 225 PC/ABS alloy Characteristics:Impact resistantHeat resistantDimensional stabilityApplications:Air con. grillAll information provided by Samyang |
|||
Volume Resistivity | 5.00e+16 ohm-cm | 5.00e+16 ohm-cm | IEC 60093 |
SABIC Innovative Plastics NORYL N1150 PPE+PS (Europe-Africa-Middle East) Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add.. |
|||
Volume Resistivity | 5.00e+16 ohm-cm | 5.00e+16 ohm-cm | IEC 60093 |
Polyplastics Duranex® 2000 Polybutylene Terephthalate (PBT), High flow DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Volume Resistivity | 5.00e+16 ohm-cm | 5.00e+16 ohm-cm | IEC 60093 |
Polyplastics Duranex® 2002 Polybutylene Terephthalate (PBT), Standard DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Volume Resistivity | 5.00e+16 ohm-cm | 5.00e+16 ohm-cm | IEC 60093 |
Polyplastics Duranex® 2002U Polybutylene Terephthalate (PBT), Weather resistance DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Volume Resistivity | 5.00e+16 ohm-cm | 5.00e+16 ohm-cm | IEC 60093 |
Polyplastics Duranex® 3105H Polybutylene Terephthalate (PBT), Standard, 15% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Volume Resistivity | 5.00e+16 ohm-cm | 5.00e+16 ohm-cm | IEC 60093 |
Polyplastics Duranex® 7390W Polybutylene Terephthalate (PBT), Super low warpage, GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Volume Resistivity | 5.00e+16 ohm-cm | 5.00e+16 ohm-cm | IEC 93 |
Wolf Kunststoff ZEDEX® ZX-324 A3A PEEK Main Characteristics: Hard; Stiff; Tough; High fatigue strength; Good water resistance; Sufficient UV and weather resistance; Flame retardant; Good machinability; FDA compliant LABS; PTFE and Silico.. |
|||
Volume Resistivity | 5.00e+16 ohm-cm | 5.00e+16 ohm-cm | IEC 93 |
Wolf Kunststoff ZEDEX® ZX-324V1T A3H PEEK Polymer, Reinforced Main Characteristics: High resilience; High elasticity; Low permanent deformation; Stress resistant; High strength at temperatures above 140 ° CApplications: Shipbuilding; Chemical Engineering; Aut.. |
|||
Volume Resistivity | 5.00e+16 ohm-cm | 5.00e+16 ohm-cm | IEC 60093 |
Polyplastics Duranex® 3300 Polybutylene Terephthalate (PBT), Standard, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Volume Resistivity | >= 5.00e+16 ohm-cm | >= 5.00e+16 ohm-cm | ISO.167 DN.53482 |
Polimersan Plastics POLIPOLEN® (Polyethylene) UHMW-PE 1000 PE 1000: Polyethylene with very high molecular weight (UHMW - PE 1000; Ultra High Molecular Weight Polyethylene). Polyethylenes with molecular weight higher than 3 million gr/mol. POLIPOLEN® PE (P.. |
|||
Volume Resistivity | 5.00e+16 ohm-cm | 5.00e+16 ohm-cm | ASTM D257 |
Samyang Triloy® 200 PC/ABS alloy General purposeCharacteristics:Impact resistantGood flowApplications:Camera partsExterior panelCluster fasciaWheel coverStructural applicationI/P. core panelHelmet shellGlove box doorCowl vent grill.. |
|||
Volume Resistivity | 5.00e+16 ohm-cm | 5.00e+16 ohm-cm | ASTM D257 |
Samyang Triloy® 210N PC/ABS alloy, Flame Retardant Characteristics:Impact resistantHeat resistantFlame retardantApplications:Cellular phoneMonitor housingCoffee makerHair dryerO/A partAll information provided by Samyang |