Polyplastics Duranex® 7390W Polybutylene Terephthalate (PBT), Super low warpage, GF filled

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified
Manufacturer Polyplastics Co.
Trade Name Duranex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyplastics Duranex® 7390W Polybutylene Terephthalate (PBT), Super low warpage, GF filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers or other inorganic filler additives. Various grades are available, including flame-retardant, reinforced, and impact-resistant grades. DURANEX®, due to its mechanical strength, heat stability, electrical resistivity and wear and abrasion-resistance, offers great potential as a well-balanced, highly reliable material, having a wide variety of applications including electronic / electro-mechanical and automobile parts and various other functional parts. DURANEX® also assures moldability, dimensional stability, glossy surfaces and various fabrication capabilities providing higher added value.Information provided by PolyPlastics.
Physical Properties Metric English Comments
Density 1.65 g/cc
0.0596 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 103 MPa
14900 psi
ISO 527-1, 2
Elongation at Break 2.0 %
2.0 %
ISO 527-1, 2
Flexural Strength 166 MPa
24100 psi
ISO 178
Flexural Modulus 9.47 GPa
1370 ksi
ISO 178
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear 30.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
16.7 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
38.9 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ISO 75-1, 2
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 5.00e+16 ohm-cm
5.00e+16 ohm-cm
IEC 60093
Surface Resistance 3.00e+16 ohm
3.00e+16 ohm
IEC 60093
Comparative Tracking Index 275 V
275 V
IEC 60112