Samyang Triloy® 220 Polymer Alloy, High Impact

Category Polymer , Thermoplastic
Manufacturer Samyang
Trade Name Triloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samyang Triloy® 220 Polymer Alloy, High Impact.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent impact, formability and weather resistance.220 is a high impact grade.Applications: Automotive instrument panels and knob typesInformation provided by Samyang.
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
Water Absorption 0.20 %
0.20 %
ASTM D570
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Melt Flow 5.0 g/10 min

@Load 5.00 kg,
Temperature 250 °C
5.0 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength 56.9 MPa
8250 psi
ASTM D638
Elongation at Break 130 %
130 %
ASTM D638
Flexural Yield Strength 79.4 MPa
11500 psi
ASTM D790
Flexural Modulus 2.16 GPa
313 ksi
ASTM D790
Izod Impact, Notched 6.37 J/cm

@Thickness 3.17 mm
11.9 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 73.0 µm/m-°C
40.6 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 115 °C
239 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Electrical Properties Metric English Comments
Volume Resistivity 5.00e+16 ohm-cm
5.00e+16 ohm-cm
ASTM D257
Dielectric Constant 3.0
3.0
ASTM D150
Dielectric Strength 25.0 kV/mm
635 kV/in
ASTM D149
Dissipation Factor 0.0090
0.0090
ASTM D150
Arc Resistance 123 sec
123 sec
ASTM D495