Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | >= 1.00e+15 ohm-cm @Temperature 20.0 °C |
>= 1.00e+15 ohm-cm @Temperature 68.0 °F |
|
Professional Plastics Kaptrex® Polyimide Film Kaptrex polyimide film provides an excellent balance of electrical, mechanical, thermal, and chemical properties over a wide range of temperatures. Kaptrex film provides excellent electrical proper.. |
|||
Volume Resistivity | >= 1.00e+15 ohm-cm @Temperature 23.0 °C |
>= 1.00e+15 ohm-cm @Temperature 73.4 °F |
IEC 60093 |
DuPont Performance Polymers Crastin® 6130 NC010 PBT
(Unverified Data**) Crastin® 6130 NC010 is an unreinforced, medium high viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by DuPont Performance Polymers |
|||
Volume Resistivity | 1.00e+15 ohm-cm @Temperature 125 °C |
1.00e+15 ohm-cm @Temperature 257 °F |
Result based on 450G |
Victrex® PEEK 600G Polyetheretherketone
(discontinued **) Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta.. |
|||
Volume Resistivity | 1.00e+15 ohm-cm @Temperature 125 °C |
1.00e+15 ohm-cm @Temperature 257 °F |
IEC 60093 |
Victrex® PEEK 150G / 151G Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c.. |
|||
Volume Resistivity | 1.00e+15 ohm-cm @Temperature 125 °C |
1.00e+15 ohm-cm @Temperature 257 °F |
IEC 60093 |
Victrex® PEEK 150G903 Black Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact compliant, colou.. |
|||
Volume Resistivity | 1.00e+15 ohm-cm @Temperature 125 °C |
1.00e+15 ohm-cm @Temperature 257 °F |
IEC 60093 |
Victrex® PEEK -HT™ G22 PolyEtherKetone, Unreinforced Product Description:High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact complia.. |
|||
Volume Resistivity | >= 1.00e+15 ohm-cm @Temperature 23.0 °C |
>= 1.00e+15 ohm-cm @Temperature 73.4 °F |
DAM; IEC 60093 |
DuPont Performance Polymers Zytel® E51HSB NC010 Nylon 66
(Unverified Data**) Zytel® E51HSB NC010 is a high molecular weight, heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Volume Resistivity | >= 1.00e+15 ohm-cm @Temperature 75.0 °C |
>= 1.00e+15 ohm-cm @Temperature 167 °F |
|
Master Bond EP17HT One component epoxy system for bonding, sealing, coating and casting Product Description: Master Bond EP17HT is an one component, heat cured epoxy system for bonding, sealing, coating and encapsulating. It features good physical properties, electrical insulation prof.. |
|||
Volume Resistivity | >= 1.00e+15 ohm-cm @Temperature 75.0 °C |
>= 1.00e+15 ohm-cm @Temperature 167 °F |
|
Master Bond EP17HT-LO One component epoxy system for bonding, sealing, coating and casting Product Description: Master Bond EP17HT-LO is a one component, heat cured epoxy system for bonding, sealing, coating and encapsulating. It features good physical properties, electrical insulation pr.. |
|||
Volume Resistivity | >= 1.00e+15 ohm-cm @Temperature 20.0 °C |
>= 1.00e+15 ohm-cm @Temperature 68.0 °F |
IEC 672-1 |
CeramTec Rubalit® A 1999.5 Alumina, 99.7% Rubalit® A 1999.5 (99.7%) is mechanically stronger, features a higher heat conductivity, and is more corrosion resistant than other aluminas. This high-purity aluminum oxide ceramic with carbon mat.. |
|||
Volume Resistivity | 1.00e+15 ohm-cm @Temperature 20.0 °C |
1.00e+15 ohm-cm @Temperature 68.0 °F |
IEC 672-1 |
CeramTec V 38 Alumina, 96.0% Al2O3-SiO2 Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures. |
|||
Volume Resistivity | 1.00e+15 ohm-cm @Temperature 220 °C |
1.00e+15 ohm-cm @Temperature 428 °F |
ASTM D257 |
DuPont™ Nomex® Type 993, 120 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications includ.. |
|||
Volume Resistivity | 1.00e+15 ohm-cm @Temperature 30.0 °C |
1.00e+15 ohm-cm @Temperature 86.0 °F |
JIS-K-6723 |
Denka VINYKON W5120 PVC, W grade for non-migratory sheath and special items A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Volume Resistivity | 1.00e+15 ohm-cm @Temperature 23.0 °C |
1.00e+15 ohm-cm @Temperature 73.4 °F |
DAM; IEC 60093 |
DuPont Performance Polymers Zytel® 7301 NC010 Nylon 6
(Unverified Data**) Zytel® 7301 NC010 is a general purpose, unlubricated polyamide 6 resin for extrusion applications.Information provided by DuPont Performance Polymers |
|||
Volume Resistivity | 1.00e+15 ohm-cm @Temperature 23.0 °C |
1.00e+15 ohm-cm @Temperature 73.4 °F |
DAM; ASTM D257 |
DuPont Performance Polymers Zytel® 77G33HS1L NC010 Nylon 612 Zytel® 77G33HS1L NC010 is a 33% glass fiber reinforced, heat stabilized polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Volume Resistivity | >= 1.00e+15 ohm-cm @Temperature 1000 °C |
>= 1.00e+15 ohm-cm @Temperature 1830 °F |
|
China-Yixing Longly Refractories Cordierite Ceramics (Heat Resistance Ceramics) LONGLY's cordierite ceramics' main crystal phrase is 2MgO-2Al2O2-5SiO2, this composition has low thermal expansion coefficient and excellent thermal shock resistance. Maximum service temperature is.. |
|||
Volume Resistivity | 1.00e+15 ohm-cm @Temperature 25.0 °C |
1.00e+15 ohm-cm @Temperature 77.0 °F |
|
Abatron AboCast 7703-21/AboCure 7703-23 (C) Epoxy Adhesive and Casting Compound AboCast 7703-21/AboCure 7703-21 is an all-purpose clear, low-viscosity, variable-ratio epoxy adhesive and casting compound for electric and structural applications. As an Adhesive: it bonds permane.. |
|||
Volume Resistivity | 1.00e+15 ohm-cm @Temperature 23.0 °C |
1.00e+15 ohm-cm @Temperature 73.4 °F |
DAM; IEC 60093 |
DuPont Performance Polymers Zytel® ST801 NC010A Nylon 66
(Unverified Data**) Zytel® ST801 is an unreinforced, super tough polyamide 66 for injection molding and extrusion. It offers outstanding break resistance over a wide temperature and humidity range and high productivit.. |
|||
Volume Resistivity | 1.00e+15 ohm-cm @Temperature 23.0 °C |
1.00e+15 ohm-cm @Temperature 73.4 °F |
DAM; ASTM D257 |
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612
(Unverified Data**) Zytel® 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Volume Resistivity | 1.00e+15 ohm-cm @Temperature 23.0 °C |
1.00e+15 ohm-cm @Temperature 73.4 °F |
DAM; IEC 60093 |
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612
(Unverified Data**) Zytel® 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Volume Resistivity | 1.00e+15 ohm-cm @Temperature 23.0 °C |
1.00e+15 ohm-cm @Temperature 73.4 °F |
ASTM D257 |
DuPont Performance Polymers Rynite® 830ER NC010 PET Rynite® 830ER is 30% glass reinforced with excellent high temperature dielectric properties. Class H (180C).Information provided by DuPont Performance Polymers |
|||
Volume Resistivity | 1.00e+15 ohm-cm @Temperature 66.0 °C |
1.00e+15 ohm-cm @Temperature 151 °F |
|
Fibre Glast 88 / 87 General Purpose Epoxy Resin and Hardener
(discontinued **) Description:#88 Epoxy Resin is a 100% reactive low viscosity liquid bisphenol-A based epoxy resin diluted with Alkyl glycidyl ether. This resin is specially designed for applications requiring low v.. |
|||
Volume Resistivity | 1.00e+15 ohm-cm @Temperature 125 °C |
1.00e+15 ohm-cm @Temperature 257 °F |
|
Victrex® PEEK 650G Polyetheretherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta.. |
|||
Volume Resistivity | 1.00e+15 ohm-cm @Temperature 23.0 °C |
1.00e+15 ohm-cm @Temperature 73.4 °F |
ASTM D257 |
DuPont Performance Polymers Rynite® 940 BK505 PET
(Unverified Data**) Rynite® 940 BK505 is a 40% mica/glass reinforced modified polyethylene terephthalate with greater strength, stiffness, and low warpage.Information provided by DuPont Performance Polymers |
|||
Volume Resistivity | 1.00e+15 ohm-cm @Temperature 125 °C |
1.00e+15 ohm-cm @Temperature 257 °F |
IEC 60093 |
Victrex® PEEK 381G Medium Viscosity Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, depth filtered granules for specialty extrusion processes, standard flow, FD.. |