3M 414DL Flexomount™ Solid Printing Tapes

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 414DL Flexomount™ Solid Printing Tapes.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Flexomount™ Solid Printing Tapes are double coated tapes designed for mounting photopolymer and rubber printing plates to flexographic printing cylinders or sleeve systems. The adhesive systems are specially formulated for clean removability from both the plate and the print cylinder. Flexomount tapes have a solid vinyl carrier which is designed for printing solids and line work.Information provided by 3M
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
Thickness 102 microns
4.00 mil
Paper Liner
102 microns
4.00 mil
Poly Liner
254 microns
10.0 mil
Tape
Mechanical Properties Metric English Comments
Peel Strength 0.3287 kN/m
1.875 pli
Composite Sleeve, Adhesion; ASTM D3330
0.438 kN/m
2.50 pli
Photopolymer, Adhesion; ASTM D3330
0.5478 kN/m
3.125 pli
Stainless Steel, Adhesion; ASTM D3330
0.5478 kN/m
3.125 pli
Rubber, Adhesion; ASTM D3330
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Adhesive Type Rubber Soft