Glass Transition Temp, Tg 54.0 °C
129 °F
TM R050-25
Resinlab® EP1225 Black Unfilled Epoxy Adhesive
Resinlab™ EP1225 Black is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. It has slightly thixotropic viscosity to give gap filling ability bust stil..
Glass Transition Temp, Tg 54.0 °C
129 °F
Ultimate Tg
Tra-Con Tra-Bond 2135D High Impact Epoxy Adhesive
TRA-BOND 2135D is a medium viscosity epoxy adhesive recommended for bonding, laminating, sealing, and structural repair applications where easy mixing and good wetting combined with high impact stre..
Glass Transition Temp, Tg 54.0 °C
129 °F
Ultimate Tg
Tra-Con Tra-Bond FDA2 Food and Drug Application Epoxy Adhesive
TRA-BOND FDA-2 is a medium viscosity epoxy resin system specifically developed for medical device applications. It has been tested in accordance with USP biological reactivity tests, in vivo and rec..
Glass Transition Temp, Tg 54.0 °C
129 °F
Ultimate Tg
Tra-Con Tra-Bond FDA2YL02 Food and Drug Application Epoxy Adhesive
TRA-BOND FDA-2 YL02 is a medium viscosity epoxy resin system specifically developed for adhesive and coating applications in accordance with Title 21, U.S. Code of Federal Regulations, Food and Drug..
Glass Transition Temp, Tg 54.0 °C
129 °F
Ultimate Tg
Tra-Con Tra-Bond 216H01 Blush-Free Non-Sag Structural Epoxy Adhesive
TRA-BOND 216H01 is a two-part epoxy adhesive specifically formulated to be non-sagging and have improved adhesion to smooth, non-porous substrates such as glass, ceramic, stainless steel, etc. This ..
Glass Transition Temp, Tg 54.0 °C
129 °F
Atom Adhesives AA-BOND FDA2 Epoxy Adhesive
AA-BOND FDA2 is a medium viscosity epoxy resin system specifically developed for medical device applications. It has been tested in accordance with USP biological reactivity tests, in vivo and recei..
Glass Transition Temp, Tg 54.0 °C
129 °F
3M Scotchcast™ 4 Electrical Insulating Resin
3M Scotchcast Electrical Insulating Resin 4 is a two-part, epoxy insulating and encapsulating resin. This resin, mixed in its unique two-part bag, generates its own heat to cure. Its compatibility w..
Glass Transition Temp, Tg 54.0 °C
129 °F
Atom Adhesives AA-SUPERTHERM 195 Epoxy Adhesive
AA-SUPERTHERM 195 is a two component, thermally conductive epoxy system recommended for staking transistors, diodes, resistors, integrated circuits and other heat sensitive components to printed cir..
Glass Transition Temp, Tg 54.0 - 60.0 °C
129 - 140 °F
Average value: 56.0 °C Grade Count:6
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min..
Glass Transition Temp, Tg 54.0 °C
129 °F
TM R050-25
Resinlab® EP1310 Medium Reactivity Epoxy Encapsulant
Resinlab™ EP1310 is a two part medium reactivity epoxy encapsulant capable of being quickly gelled prior to full cure by exposing to a UV light source. Usually 5- 10 seconds is sufficient to gel th..
Glass Transition Temp, Tg 53.9 °C
129 °F
Tg tan d, 60°C/140°F-95%RH, 30days; Cured Neat Resin Property, 1 hour @ 70°C/158°F
Hexcel® Redux® 810 Two-Part Epoxy Paste Adhesive
Redux® 810 is a multi-purpose, high shear and peel strength, two-part, toughened epoxy paste adhesive with corrosion-inhibiting properties.Features: Available in cartridges with a static mixer and ..