3M Scotchkote™ 474 Epoxy Concrete Repair

Category Polymer , Thermoset , Epoxy
Manufacturer 3M
Trade Name Scotchkote™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotchkote™ 474 Epoxy Concrete Repair.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Scotchkote Epoxy Concrete Repair 474 has been specifically developed as a three component 100% solids high performance mortar for use as a heavy duty repair system for concrete surfaces.Product Features:Combines good application characteristics with excellent chemical resistanceDesigned for application by trowel or floatNo shrinkage or volume change during cureHigh abrasion resistance and excellent adhesionUnaffected by most industrial chemicalsInformation provided by 3M
Physical Properties Metric English Comments
Solids Content 100 %
100 %
Volatile Organic Compounds (VOC) Content 0.00 g/l
0.00 g/l
Thickness 6100 microns
240 mil
Mechanical Properties Metric English Comments
Compressive Strength 86.2 MPa
12500 psi
ASTM D695
Impact Test 1.80 J
1.33 ft-lb
ASTM D256
Abrasion 145
145
[mg] 1 kg, CS17; ASTM D4060
Processing Properties Metric English Comments
Cure Time 480 min
8.00 hour
Hard Dry
1440 min
24.0 hour
Full Hardness
10100 min
168 hour
Full Cure
Descriptive Properties Value Comments
Appearance Light Gray