Processing Properties Metric English Comments
Cure Time 480 min
8.00 hour
Full cure
Resinlab® CYNERGY CA6907 Adhesive
Description: The CYNERGY 6900 SERIES are for use in demanding applications where very fast cure speeds and high temperature resistance are required. These are single component solvent free materials..
Cure Time 480 min
8.00 hour
(overnight), For service (Depends on temperature and porosity of wood being treated).
Protective Coating PC-Petrifier® Wood Hardener
Description: PC-Petrifier® is great for sealing and restoring rotted soft wood fibers found in window sills, sashes, frames, trim, beams and columns, fences, decks, paneling, flooring, log homes, p..
Cure Time 480 min
8.00 hour
Full cure
Resinlab® CYNERGY CA6003 Adhesive
Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety..
Cure Time 480 min
8.00 hour
Full cure
Resinlab® CYNERGY CA6012 Adhesive
Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety..
Cure Time 480 min
8.00 hour
Full cure
Resinlab® CYNERGY CA6014 Adhesive
Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety..
Cure Time 480 min
8.00 hour
Full cure
Resinlab® CYNERGY CA6101 Adhesive
Description: The CYNERGY 6100 SERIES products are used to bond metal to itself or other substrates. It is available in five standard viscosities.Application: The CYNERGY SERIES of the cyanoacrylates..
Cure Time 480 min
8.00 hour
Full cure
Resinlab® CYNERGY CA6103 Adhesive
Description: The CYNERGY 6100 SERIES products are used to bond metal to itself or other substrates. It is available in five standard viscosities.Application: The CYNERGY SERIES of the cyanoacrylates..
Cure Time 480 min
8.00 hour
Full cure
Resinlab® CYNERGY CA6403 Adhesive
Description: The CYNERGY 6400 SERIES are clear, highly toughened, high peel strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. They impa..
Cure Time 480 min
8.00 hour
Full cure
Resinlab® CYNERGY CA6703 Adhesive
Description: The CYNERGY 6700 SERIES are modified to provide greatly reduced odor and a further reduction of bloom or frosting of plastics when compared to the 6600 Series. These products are ideal ..
Cure Time 480 min
8.00 hour
Full Cure
Resinlab® RC8038 Anaerobic Retaining Compound
The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products ..
Cure Time 480 min
8.00 hour
Full Cure
Resinlab® RC8040 Anaerobic Retaining Compound
The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products ..
Cure Time 480 min
8.00 hour
Full Cure
Resinlab® RC8048 Anaerobic Retaining Compound
The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products ..
Cure Time 480 min
8.00 hour
Full Cure
Resinlab® RC8075 Anaerobic Retaining Compound
The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products ..
Cure Time 480 min
8.00 hour
Full cure
Resinlab® CYNERGY CA6802 Adhesive
Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP ..
Cure Time 480 min
8.00 hour
Full cure
Resinlab® CYNERGY CA6804 Adhesive
Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP ..
Cure Time 480 min
8.00 hour
Full cure
Resinlab® CYNERGY CA6805 Adhesive
Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP ..
Cure Time 480 min
8.00 hour
Full cure
Resinlab® CYNERGY CA6806 Adhesive
Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP ..
Cure Time 480 - 960 min
8.00 - 16.0 hour
Lord Adhesives 3170 Two-component, high cold strength, cryogenic application Epoxy Adhesive
Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh..
Cure Time 480 min
8.00 hour
Lord Adhesives 370 Two Component Epoxy Adhesive
Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh..
Cure Time 480 min
8.00 hour
Tack-Free Time
3M AC-236 Class B-1/2 Aerospace Sealant
3M Aerospace Sealant AC-236 Class B are two-component, manganese dioxide cured, liquid polysulfide polymer system providing excellent fuel tank and fuselage seals. They have outstanding resistance t..
Cure Time 480 min
8.00 hour
Tack-Free Time
3M AC-251 Gray Class B-2 Aerospace Sealant
3M Aerospace Sealant AC-251 Gray Class B are two-part, quick curing, polysulfide based canopy and windshield sealants. These products are formulated for sealing acrylic, glass, and polycarbonate air..
Cure Time 480 - 720 min
8.00 - 12.0 hour
Tack Free Time, catalyzed with QM CAT SKIN 30
ACC QM Skin 30 QSI Quantum Silicones 30 Durometer Condensation Cure moldmaking Material
QM Skin 30 is a two-component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and very low bleed in addition to good shelf-l..
Cure Time 480 - 720 min
8.00 - 12.0 hour
Time to Handling Strength
3M Scotch-Weld™ DP190 Gray Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP190 Gray is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Gray and exhibits good peel, shear and environmental aging properties.Information pro..
Cure Time 480 - 1440 min
8.00 - 24.0 hour
Full Cure
3M Scotch-Weld™ DP8010NS Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010NS is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polyprop..
Cure Time 480 min
8.00 hour
3M Scotch-Weld™ 3549 B/A Two-Part Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie..
Cure Time 480 min
8.00 hour
Full Cure
Resinlab® RC8009 Anaerobic Retaining Compound
The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products ..
Cure Time 480 min
8.00 hour
Full Cure
Resinlab® TL5090 Anaerobic Threadlocking Compound
The TL5000 Series anaerobic threadlocking compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. They form a ..
Cure Time 480 - 720 min

@Temperature 24.0 °C
8.00 - 12.0 hour

@Temperature 75.2 °F
BCC Products BC 5010 Epoxy Laminating System
BC 5010 is a high quality, low viscosity room temperature curing laminating resin. A Safety System for the production of a variety of dimensionally stable fiberglass tools. BC 5010 features low odor..
Cure Time 480 - 720 min
8.00 - 12.0 hour
Time to Handling Strength
3M Scotch-Weld™ 2216 B/A Tan NS Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel..
Cure Time 480 min
8.00 hour
Full cure
Resinlab® CYNERGY CA6903 Adhesive
Description: The CYNERGY 6900 SERIES are for use in demanding applications where very fast cure speeds and high temperature resistance are required. These are single component solvent free materials..