Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.67 g/cc | 1.67 g/cc | ASTM D792 |
Nylene® Vexel™ B12GF45 SA , 45% Glass Reinforced PBT Description: Vexel™ B12GF45 SA is a 45% glass fiber reinforced PBT with improved surface aPolyphenylene Etherarance. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are.. |
|||
Specific Gravity | 1.67 g/cc | 1.67 g/cc | ASTM D 792 |
RTP Company RTP 1305 TFE 15 Z Polyphenylene Sulfide (PPS), Glass Fiber - PTFE Lubricated - FDA Compliant Ingredients
&a Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade. |
|||
Specific Gravity | 1.67 g/cc | 1.67 g/cc | Method A; ASTM D792 |
LNP Lubricomp® PDX-O-90351 Polyphenylene Sulfide, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Specific Gravity | 1.67 g/cc | 1.67 g/cc | ASTM D792 |
PolyOne Maxxam™ FR PO Conc 62 Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Specific Gravity | 1.67 g/cc | 1.67 g/cc | ASTM D792 |
RTP Company RTP 4005 FR Polyphthalamide (PPA) Glass Fiber 30% - Flame Retardant
(discontin Glass Fiber 30% - Flame RetardantComments:Glass FiberFlame RetardantUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information .. |
|||
Specific Gravity | 1.67 g/cc | 1.67 g/cc | ASTM D792 |
RTP Company RTP 2208 LF Polyetheretherketone (PEEK) Glass Fiber 45% - Low Flow
(discontinu Glass Fiber 45% - Low FlowComments:Glass FiberLow FlowUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RT.. |
|||
Specific Gravity | 1.67 g/cc | 1.67 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1301-0793 PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. .. |
|||
Specific Gravity | 1.67 g/cc | 1.67 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1301-8331-2 PPS, linear, with glass fiber, thermally conductive modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.Low warpage, isotropic shrinkage characteristics.Coil formers, duty parts in p.. |
|||
Specific Gravity | 1.67 g/cc | 1.67 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1301-8524 PPS, linear, with glass fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Specific Gravity | 1.67 g/cc | 1.67 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 3-8437 Polyamide 6, with glass fiber Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts with low creep.Emergency running property.Suitable for metall inserts.Control.. |
|||
Specific Gravity | 1.67 g/cc | 1.67 g/cc | ISO 1183 |
Gromax BFG50-FU00B3 Nylon 6 49.4% Glass Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Specific Gravity | 1.67 g/cc | 1.67 g/cc | ISO 1183 |
Gromax BFG50-FU00B3 Nylon 6 49.4% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Specific Gravity | 1.67 - 1.71 g/cc | 1.67 - 1.71 g/cc | ASTM D792 |
Loxim 235 01V0 Polybutylene Terephthalate Information provided by Loxim Industries |
|||
Specific Gravity | 1.67 g/cc | 1.67 g/cc | ASTM D792 |
SABIC Innovative Plastics ULTEM 4000 PEI (Asia Pacific) Glass fiber, PTFE, and Graphite filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 listing. |
|||
Specific Gravity | 1.67 g/cc | 1.67 g/cc | ASTM D792 |
SABIC Innovative Plastics Valox® 4631 PBT (Europe-Africa-Middle East) VALOX 4631 is a 30% glass reinforced, flame retarded PBT injection moulding resin with good electrical properties and excellent mechanical properties. |
|||
Specific Gravity | 1.67 g/cc | 1.67 g/cc | ASTM D792 |
Shinkong Synthetic Fibers Shinite® N602G6S Nylon 66, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Specific Gravity | 1.67 g/cc | 1.67 g/cc | ASTM D792 |
A. Schulman ComAlloy® E-13086 Glass/TFE Reinforced PPS Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Specific Gravity | 1.67 g/cc | 1.67 g/cc | ASTM D792 |
A. Schulman COMTUF® 464 Glass Reinforced Impact Modified PBT Alloy Information provided by A. Schulman. |
|||
Specific Gravity | 1.67 g/cc | 1.67 g/cc | ASTM D792 |
A. Schulman ComAlloy® E-13086 Glass/TFE Reinforced PPS Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Specific Gravity | 1.67 g/cc | 1.67 g/cc | ASTM D 792 |
RTP Company RTP 1305 TFE 15 P-1 Polyphenylene Sulfide (PPS), Glass Fiber Reinforced - PTFE Lubricated |
|||
Specific Gravity | 1.67 g/cc | 1.67 g/cc | ASTM D792 |
A. Schulman ComAlloy® E-13086 Glass/TFE Reinforced PPS Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Specific Gravity | 1.67 g/cc | 1.67 g/cc | ASTM D792 |
A. Schulman COMTUF® 464 Glass Reinforced Impact Modified PBT Alloy Information provided by A. Schulman. |
|||
Specific Gravity | 1.67 g/cc | 1.67 g/cc | ASTM D 792 |
RTP Company RTP 2307 A TFE 15 Rigid Thermoplastic Polyurethane (RTPU), Glass Fiber - PTFE Lubricated |
|||
Specific Gravity | 1.67 g/cc | 1.67 g/cc | ASTM D792 |
A. Schulman COMTUF® 464 Glass Reinforced Impact Modified PBT Alloy Information provided by A. Schulman. |
|||
Specific Gravity | 1.67 g/cc | 1.67 g/cc | ASTM D792 |
E-Polymers SEPAZ® K140HF 40% Glass Fiber Reinforced Low Flash, High Flow PPS Resin Polyphenylene Sulfide Resin: High-performance engineering plastic SEPAZ PPS boasts excellent high-temperature resistance, flame retardancy and chemical resistance, physical strength, and its fluidit.. |
|||
Specific Gravity | 1.67 g/cc | 1.67 g/cc | |
BCC Products BC 7136-2 Epoxy Casting BC7136-2 is an aluminum filled thick section casting system with heat resistance to 300ºF. May be cast to a thickness of 2 inches in non-conductive molds, 3 inches in conductive molds and thicker s.. |
|||
Specific Gravity | 1.67 - 1.73 g/cc | 1.67 - 1.73 g/cc | NBR NM-IEC 60811-1-3 |
Karina 38/49-FC-LMP Straw Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.67 g/cc | 1.67 g/cc | ASTM D792 |
Techmer Lehvoss Compounds Luvotech™ J-1305/40 BK5011 PPS
(discontinued **) Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated. |