Material Notes:
Data provided by the manufacturer, ComAlloy International Company.45% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Ultimate 202 MPa
29300 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Strength 322 MPa
46700 psi
ASTM D790
Flexural Modulus 12.5 GPa
1810 ksi
ASTM D790
Izod Impact, Notched 1.76 J/cm
3.30 ft-lb/in
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D256
Thermal Properties Metric English Comments
Melting Point 205 - 225 °C
401 - 437 °F
Deflection Temperature at 0.46 MPa (66 psi) 230 °C
446 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 214 °C
417 °F
ASTM D648
Processing Properties Metric English Comments
Middle Barrel Temperature 260 - 271 °C
500 - 520 °F