Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman ComAlloy Voloy® 112 Polypropylene, Glass Reinforced, Chemically Coupled, Flame Retardant, UL

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer A. Schulman ComAlloy
Trade Name Voloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman ComAlloy Voloy® 112 Polypropylene, Glass Reinforced, Chemically Coupled, Flame Retardant, UL.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, ComAlloy International Company.15% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 107
107
ASTM D785
Tensile Strength, Ultimate 61.0 MPa
8850 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Strength 85.0 MPa
12300 psi
ASTM D790
Flexural Modulus 6.20 GPa
899 ksi
ASTM D790
Izod Impact, Notched 0.690 J/cm
1.29 ft-lb/in
ASTM D256
Izod Impact, Unnotched 3.10 J/cm
5.81 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 159 °C
318 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 136 °C
277 °F
ASTM D648
Processing Properties Metric English Comments
Middle Barrel Temperature 229 - 246 °C
444 - 475 °F