Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman POLYFORT™ FXP 3000-3120 Glass Sphere Filled Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Glass Bead Filled
Manufacturer A. Schulman, Inc.
Trade Name POLYFORT™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYFORT™ FXP 3000-3120 Glass Sphere Filled Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolyfort® FXP 3000-3120 is a 30% glass sphere filled copolymer polypropylene compound.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Melt Flow 18 g/10 min
18 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 18.0 MPa
2610 psi
ASTM D638
Elongation at Break 60 %
60 %
ASTM D638
Flexural Modulus 1.60 GPa
232 ksi
ASTM D790
Izod Impact, Notched 0.250 J/cm
0.468 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °C
190 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 56.0 °C
133 °F
ASTM D648