Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman PP 1452 Polypropylene Medium Impact Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer A. Schulman, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman PP 1452 Polypropylene Medium Impact Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolypropylene PP 1452 is a medium impact polypropylene with a good balance of stiffness and impact resistance. It is stabilized for heat stability, and is chemical resistant.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.902 g/cc
0.902 g/cc
ASTM D792
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 70
70
ASTM D785
Tensile Strength, Yield 25.9 MPa
3750 psi
at 2 in/min; ASTM D638
Elongation at Yield 15 %
15 %
ASTM D638
Flexural Modulus 1.14 GPa
165 ksi
ASTM D790
Izod Impact, Notched 16.0 J/cm
30.0 ft-lb/in
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D256
Gardner Impact 22.71 J
16.75 ft-lb
ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
ASTM D648
Users viewing this material also viewed the following: