Material Notes:
Uses: Weld wire, woven wire mesh belts, rod for heat treat baskets, heat treat fixtures.Property values are for samples in the metallurgical condition: As rolled.Information provided by Allvac, An Allegheny Teledyne Company.
Physical Properties Metric English Comments
Density 8.00 g/cc
0.289 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 80
80
Tensile Strength, Ultimate 586 MPa
85000 psi
Tensile Strength, Yield 276 MPa

@Strain 0.200 %
40000 psi

@Strain 0.200 %
Elongation at Break 40 %
40 %
Reduction of Area 70 %
70 %
Component Elements Properties Metric English Comments
Carbon, C 0.040 %
0.040 %
Chromium, Cr 18.5 %
18.5 %
Copper, Cu 0.50 %
0.50 %
Iron, Fe 43 %
43 %
as balance
Lead, Pb 0.0010 %
0.0010 %
Manganese, Mn 1.0 %
1.0 %
Nickel, Ni 35.5 %
35.5 %
Phosphorous, P 0.010 %
0.010 %
Silicon, Si 1.13 %
1.13 %
Sulfur, S 0.010 %
0.010 %
Tin, Sn 0.010 %
0.010 %