Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.00 g/cc | 0.289 lb/in³ | RT |
Outokumpu 4404 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | RT |
Outokumpu 4439 Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), and cold rolled strip/sheet forms. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | theoretical |
Kennametal Stellite Deloro® 711 PM after P/M Processing Deloro 711 is currently being developed. Adhesive wear test data: P/M 0.1, cast 0.1; Abrasive wear test data P/M 6 mm^3, cast 26 mm^3. Typical applications include vane plugs, fuel metering pins, sp.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
Industeel CLC 18.15.4L 3% Mo Minimum Austenitic Stainless Steel Description: CLC 18-15-4L (317L) is an austenitic stainless steel with a 3% minimum Molybdenum addition. Alloys CLC 18-15-4L (317L) exhibit austenitic microstructure free of deleterious carbide prec.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
Industeel SIRIUS 800 H+ Heat Resistant Alloy Description: The SIRIUS® 800, H and H+ grades are three variants of a high chromium and nickel austenitic alloy which combines good corrosion and creep resistance. SIRIUS® 800 is employed at t.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
Lucas-Milhaupt FOS FLO 7 Copper Phosphorus Alloy Applications:Fos-Flo 7 is a low cost brazing filler metal suitable for joining copper to copper and copper to copper alloys where critical impact or vibration stresses are not encountered in service.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
Lucas-Milhaupt Silvalite Brazing Alloy SILVALITE is used for the brazing of copper and copper alloys, brass and bronze. It can also be used on silver, tungsten and molybdenum. It is primarily used for the joining of copper-to-copper on v.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
Lucas-Milhaupt Silvaloy® 0 Brazing Alloy Silvaloy 0 is used for the brazing of copper and copper alloys, brass and bronze. It can also be used on silver, tungsten and molybdenum. It is primarily used for the joining of copper-to-copper on .. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
Latrobe Marvac 250 VIM-VAR ; 5 in. High Strength Maraging Steel MARVAC 250 VIM-VAR is a low carbon maraging steel capable of 240,000 psi minimum yield strength, coupled with excellent toughness and ductility. The alloy has good fabrication characteristics, which.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
Indium Corp. Indalloy 110 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
Special Metals INCOLOY® alloy 028 Austenitic Stainless Steel INCOLOY® alloy 028 (UNS N08028/W. Nr. 1.4563) is a highly alloyed austenitic stainless steel offering resistance to a variety of corrosive media. By virtue of its contents of chromium and molybd.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
Special Metals UDIMAR® alloy 300 Fe-Ni Maraging Steel UDIMAR® alloy 300 (UNS K93120) is an age-hardenable (maraging) iron-nickel steel combining ultra-high strength, toughness and resistance to crack propagation. The alloy is well suited to applica.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
Alloy Wire International RW 70 Hot Cutting Wire - High Strength Maintains high strength at elevated temperatures. Used for cutting expanded polystyrene (EPS) foam and for the heat sealing of polypropylene bags.Information provided by Alloywire International. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel-Molybdenum 317L (UNS S31703) Allegheny Ludlum's 317L™ is molybdenum-bearing austenitic stainless steel with greatly increased resistance to chemical attack as compared to the conventional chromium-nickel austenitic stainless s.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel-Molybdenum 317LX™ (UNS S31725) Allegheny Ludlum's 317LX™ is molybdenum-bearing austenitic stainless steel with greatly increased resistance to chemical attack as compared to the conventional chromium-nickel austenitic stainless .. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
ATI Allvac® 330 UNS N08330 Nickel Superalloy Uses: Weld wire, woven wire mesh belts, rod for heat treat baskets, heat treat fixtures.Property values are for samples in the metallurgical condition: As rolled.Information provided by Allvac, An A.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
ATI Allvac® VascoMax® C-300 Specialty Steel, Heat Treatment: 927°C (1700°F) + Age Data provided by Allvac.Applications: Missile components, jet engine shafts. Spring wire for valve springs in high-performance internal combustion engines. |