ATI Allvac® Nickelvac® X- 751 UNS N07751 Nickel Superalloy

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer ATI Allvac
Trade Name Nickelvac®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allvac® Nickelvac® X- 751 UNS N07751 Nickel Superalloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Uses: Components for gas turbine engines, exhaust valve stock for internal combustion engines.Property values are for samples in the metallurgical condition: 1800°F age.Information provided by Allvac, An Allegheny Teledyne Company.
Physical Properties Metric English Comments
Density 8.24 g/cc
0.298 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 35
35
Tensile Strength, Ultimate 1310 MPa
190000 psi
Tensile Strength, Yield 965 MPa

@Strain 0.200 %
140000 psi

@Strain 0.200 %
Elongation at Break 22 %
22 %
Reduction of Area 20 %
20 %
Component Elements Properties Metric English Comments
Aluminum, Al 1.2 %
1.2 %
Carbon, C 0.050 %
0.050 %
Chromium, Cr 15.5 %
15.5 %
Copper, Cu 0.20 %
0.20 %
Iron, Fe 7.0 %
7.0 %
Manganese, Mn 0.50 %
0.50 %
Nickel, Ni 70 %
70 %
Niobium, Nb (Columbium, Cb) 1.1 %
1.1 %
Silicon, Si 0.20 %
0.20 %
Sulfur, S 0.0050 %
0.0050 %
Titanium, Ti 2.3 %
2.3 %