Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 965 MPa | 140000 psi | |
Performance Alloys MoldStar® 90 Copper Mold Alloy Description: MoldStar® 90 is a beryllium-free copper alloy for the blow molding and injection molding industries as well as other industrial applications. MoldStar® 90 provides a good balance of t.. |
|||
Tensile Strength, Yield | 965 MPa | 140000 psi | |
Meehanite K-405 Austempered Ductile Iron Type K-405 is for applications involving wear and requiring high tensile and endurance limit. Excellent founding properties enable more accurate castings with savings in machine stock required. Da.. |
|||
Tensile Strength, Yield | >= 965 MPa | >= 140000 psi | |
MetalTek IN® 909 Centri-Vac Nickel Cobalt Based Alloy Information provided by MetalTek |
|||
Tensile Strength, Yield | 965 MPa | 140000 psi | |
Latrobe Lesco 53 VIM-VAR Premium Carburizing Steel LESCO 53 VIM-VAR is a premium quality alloy carburizing gear steel designed to resist softening at elevated service temperatures. It is double vacuum processed by vacuum induction melting followed .. |
|||
Tensile Strength, Yield | 965 MPa @Strain 0.200 % |
140000 psi @Strain 0.200 % |
|
Haynes 625 alloy, 20% cold reduction Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Tensile Strength, Yield | 965 - 1096 MPa @Strain 0.200 % |
140000 - 159000 psi @Strain 0.200 % |
|
Latrobe Lescalloy® Jethete M-152 ESR 8" RCS High Strength Stainless Steel LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800Â.. |
|||
Tensile Strength, Yield | 965 MPa | 140000 psi | |
HP Alloys Alloy 718, 20% Cold Worked 20% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
Tensile Strength, Yield | >= 965 MPa @Strain 0.200 % |
>= 140000 psi @Strain 0.200 % |
|
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5), Rod, Square, or Hex, >1.500-2.000 in, Per Mil-T-9047G Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Rod, Square, or Hex, >1.500-2.000 in, Per Mil-T-9047G; other specific form/thickness entries are .. |
|||
Tensile Strength, Yield | >= 965 MPa | >= 140000 psi | 0.2% Offset |
Eagle Brass 301 Austenitic Stainless Steel, Full Hardened Type 301 is a chromium-nickel stainless steel that provides high strength and good ductility with chromium and nickel contents lowered to increase the work hardening range. This permits higher tens.. |
|||
Tensile Strength, Yield | >= 965 MPa | >= 140000 psi | 0.2% Offset |
Eagle Brass 302 Austenitic Stainless Steel, Full Hardened Types 302 is a widely used variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled.Information provided by Eagle Brass Compa.. |
|||
Tensile Strength, Yield | >= 965 MPa | >= 140000 psi | 0.2% Offset |
Eagle Brass 304L Austenitic Stainless Steel, Full Hardened Type 304L is a very common variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled. Lower carbon 304L minimizes chromium ca.. |
|||
Tensile Strength, Yield | >= 965 MPa | >= 140000 psi | 0.2% Offset |
Eagle Brass 316 Austenitic Stainless Steel, Full Hardened The Mo addition increases general corrosion resistance to pitting from chloride ion solutions, and provides increased strength at elevated temperatures. Properties are similar to those of Type 304 .. |
|||
Tensile Strength, Yield | >= 965 MPa | >= 140000 psi | 0.2% Offset |
Eagle Brass 316L Austenitic Stainless Steel, Full Hardened Type 316L is an extra-low carbon version of Type 316 that minimizes carbide precipitation. Typical uses include exhaust manifolds, furnace parts, heat exchangers, jet engine parts, pharmaceutical a.. |
|||
Tensile Strength, Yield | 965 - 1030 MPa @Strain 0.200 % |
140000 - 150000 psi @Strain 0.200 % |
|
Crucible Steel Maxel® 2000 Stainless Steel Maxel 2000 is a free-machining stainless holder block steel which is based on the nominal analysis of Type 414L rather than Type 420. It is supplied pre-hardened to about HRC 37. Due to its unique c.. |
|||
Tensile Strength, Yield | >= 965 MPa | >= 140000 psi | 0.2% Offset |
Eagle Brass 304 Austenitic Stainless Steel, Full Hardened Types 304 is a widely used variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled.Information provided by Eagle Brass Compa.. |
|||
Tensile Strength, Yield | 966 MPa @Strain 0.200 % |
140000 psi @Strain 0.200 % |
|
ATI Allvac® 6-2-4-2 Titanium Alloy, Heat Treatment: 982°C (1800°F) + Age Data provided by Allvac.Applications: High-temp jet engines. Blades, discs, spacers, seals. High performance automotive valves. Standard, rotor/premium grades. |
|||
Tensile Strength, Yield | 966 MPa @Strain 0.200 % |
140000 psi @Strain 0.200 % |
|
ATI Allvac® 6-2-4-2-Si UNS R54620 modified Titanium Alloy Uses: High performance valves for internal combustion engines. Aerospace and commercial grades.Property values are for samples in the metallurgical condition: 1800°F anneal.Information provided by .. |
|||
Tensile Strength, Yield | 966 MPa @Strain 0.200 % |
140000 psi @Strain 0.200 % |
|
ATI Allvac® 8-1-1 Titanium Alloy, Heat Treatment: 982°C (1800°F) + Age Data provided by Allvac.Applications: Fan & compressor blades, discs, spacers, seals, rings. Excellent creep resistance. Standard, rotor/premium grades. |
|||
Tensile Strength, Yield | 966 MPa @Strain 0.200 % |
140000 psi @Strain 0.200 % |
|
ATI Allvac® Grade 15-3-3-3 UNS R58153 Titanium Alloy Metastable beta titanium alloy. Uses: Industrial and aerospace components, pressure vessels, fittings, tubing, fasteners.Property values are for samples in the metallurgical condition: 1600°F annea.. |
|||
Tensile Strength, Yield | 965 MPa @Strain 0.200 % |
140000 psi @Strain 0.200 % |
|
ATI Allvac® Nickelvac® 80 A UNS N07080 Nickel Superalloy Uses: Components for gas turbine engines, exhaust valve stock for internal combustion engines, high temperature bolts & fasteners.Property values are for samples in the metallurgical condition: 1700.. |
|||
Tensile Strength, Yield | 966 MPa | 140000 psi | 0.2% Offset |
ATI Allvac® Nickelvac® TJA-1537™ UNS R31537 & UNS R31538 Nickel Superalloy Cobalt-base alloy for machined and forged medical and surgical devices requiring high fatigue strength; total joint replacement.Property values are for samples in the metallurgical condition: Warm w.. |
|||
Tensile Strength, Yield | 965 MPa @Strain 0.200 % |
140000 psi @Strain 0.200 % |
|
ATI Allvac® Nickelvac® X- 751 UNS N07751 Nickel Superalloy Uses: Components for gas turbine engines, exhaust valve stock for internal combustion engines.Property values are for samples in the metallurgical condition: 1800°F age.Information provided by Allv.. |
|||
Tensile Strength, Yield | 966 MPa @Strain 0.200 % |
140000 psi @Strain 0.200 % |
|
ATI Allvac® Vasco® 450 Specialty Steel, Heat Treatment: 1038°C (1900°F) + Age Data provided by Allvac.Applications: Land-based turbine blades and buckets. |
|||
Tensile Strength, Yield | 966 MPa @Strain 0.200 % |
140000 psi @Strain 0.200 % |
|
ATI Allvac® Vasco® M152 Specialty Steel, Heat Treatment: 691°C (1275°F) Anneal Data provided by Allvac.Applications: Rings and structural components for land-based turbines. |
|||
Tensile Strength, Yield | 965 MPa @Strain 0.200 %, Temperature 316 °C |
140000 psi @Strain 0.200 %, Temperature 601 °F |
|
Carpenter Custom 450® Stainless Steel, Condition H950 (Age Hardened 510°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
Tensile Strength, Yield | 965 MPa @Strain 0.200 %, Temperature -73.0 °C |
140000 psi @Strain 0.200 %, Temperature -99.4 °F |
|
Carpenter Gall-Tough PLUS™ Stainless, Annealed, 30% Cold Work Data provided by Carpenter Technology Corporation.Annealed 1150°C, water quenched, and cold drawn.Threshold Galling Stress 48 MPa. The avg. total volume loss on the wear test is 10.6 mm³ at 100 r.. |
|||
Tensile Strength, Yield | >= 965 MPa @Strain 0.200 % |
>= 140000 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum Stainless Steel Type 301, Full Hard (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |
|||
Tensile Strength, Yield | 965 MPa @Temperature 22.0 °C |
140000 psi @Temperature 71.6 °F |
Hardened and tempered to 34 HRC |
Schmolz + Bickenbach Formadur® 2085 Plastic Mold Steel Description: FORMADUR 2085 is a free-machining corrosion-resistant mold frame steelCharacteristics: Lower mold production costs due to improved machinability; Improved corrosion resistance compared .. |
|||
Tensile Strength, Yield | 965 MPa | 140000 psi | Offset not given |
Carpenter Pyrowear® 53 Tool Steel, Core Tensile Properties Data provided by Carpenter Technology Corporation.This is a carburizing steel possessing good temper resistance and high case hot hardness while maintaining high core impact strength and fracture to.. |