Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aaron Industries AVPE HD 300-3 MELT 20 Virgin Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Blow Molding Grade
Manufacturer Aaron Industries Corporation
Trade Name AVPE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aaron Industries AVPE HD 300-3 MELT 20 Virgin Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A natural HDPE resin, specifically designed for high speed blow molding and extrusion applications.
Physical Properties Metric English Comments
Specific Gravity 0.955 g/cc
0.955 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM D955
Melt Flow 20 g/10 min

@Load 5.00 kg,
Temperature 190 °C
20 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.2 MPa
3800 psi
ASTM D638
Flexural Modulus 2.21 GPa
320 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 85.0 °C
185 °F
ASTM D1525