Abatron AboWeld 8709-18/AboCure 50-12 Nickel-Filled Electrically Conductive Epoxy Compound

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy, Electrically Conductive
Manufacturer Abatron
Trade Name AboWeld
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron AboWeld 8709-18/AboCure 50-12 Nickel-Filled Electrically Conductive Epoxy Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AboWeld 8709-18/AboCure 50-12 is a practically solventless nickel-epoxy adhesive and resurfacing system with good coating capabilities in the intermediate conductivity range. It is very versatile.
Physical Properties Metric English Comments
Solids Content 98 %
98 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 90.0 °C
194 °F
Electrical Properties Metric English Comments
Surface Resistivity per Square <= 0.60 ohm
<= 0.60 ohm
Processing Properties Metric English Comments
Cure Time 30.0 - 180 min

@Temperature 50.0 - 100 °C
0.500 - 3.00 hour

@Temperature 122 - 212 °F
>= 1440 min

@Temperature 22.0 - 30.0 °C
>= 24.0 hour

@Temperature 71.6 - 86.0 °F
Pot Life 400 min
400 min
Descriptive Properties Value Comments
Color Gray
Metal (%) 76.5
of vehicle
Parts by Weight (pbw) 100
AboWeld 8709-18
2.6
AboCure 50-12
Viscosity Paste