Adamas Adalon® 205 PTFE, 15/5% Glass/MoS2 Filled

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Glass Filled, Molded
Manufacturer Adamas
Trade Name Adalon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Adamas Adalon® 205 PTFE, 15/5% Glass/MoS2 Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Adamas, HPM
Physical Properties Metric English Comments
Specific Gravity 2.26 - 2.28 g/cc
2.26 - 2.28 g/cc
ASTM D792
Deformation 5.3 - 6.5 %
5.3 - 6.5 %
Permanent deformation after 24 hrs @ 23°C; ASTM D621
10 - 12 %
10 - 12 %
ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 55 - 59
55 - 59
ASTM D2240
Ball Indentation Hardness 42.0 - 46.0 MPa
6090 - 6670 psi
ISO 2032-N132
Tensile Strength at Break >= 18.0 MPa
>= 2610 psi
ASTM D4894
Elongation at Break >= 200 %
>= 200 %
ASTM D4894
Coefficient of Friction, Dynamic 0.080 - 0.12
0.080 - 0.12
ASTM D1894
Coefficient of Friction, Static 0.10 - 0.15
0.10 - 0.15
ASTM D1894
Thermal Properties Metric English Comments
Melting Point 327 °C
621 °F
DSC
Maximum Service Temperature, Air 260 °C
500 °F
DSC
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
DSC
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
ASTM D257
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
ASTM D257