Material Notes:
Fields of application: Foamed products of Polyolefin and other polymers.Examples: Extruded sheets and foams in general as well as injection molded parts that require a foamed core.Mode of action and advantages: ADD-VANCE® BA 401 contains a proprietary combination of endothermic blowing agent additives. ADD-VANCE® BA 401 contains a relatively high level of active components and NO polymer carrier. Please note: processing temperature and other processing conditions are a major factor to achieve a certain development of foam in the product. As a result we recommend to experiment with several processing conditions.Advantages: Universal blowing agent for Polyolefins and other polymers (e.g. Polyamide); Excellent foam development and fine cell structure; Cost savings due to reduced polymer use; Weight reduction of the final part; Cost efficient: the product is very effective at low dosing rates: 1.0 – 2.0 wt%; Foam densities of 0.5 – 0.6 g / dm3 can be achieved in Polyolefins applying processing temperatures in the range 180- 200 °C, also dependent on other conditions, such a residence time and processing pressures; and Easy to use.Information provided by ADDCOMP
Physical Properties Metric English Comments
Bulk Density 0.800 - 0.900 g/cc
0.0289 - 0.0325 lb/in³
Processing Properties Metric English Comments
Processing Temperature <= 300 °C
<= 572 °F
Descriptive Properties Value Comments
Appearance White/off-white granules
Dosing Level 1-2%
Foam densities 0.5-0.6 g/dm3