Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | |
Nabaltec NABALOX® NO 115P Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | 0.800 - 1.00 g/cc | 0.0289 - 0.0361 lb/in³ | |
Nabaltec NABALOX® NO 201 Calcined Aluminum Oxide NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | 0.800 - 1.00 g/cc | 0.0289 - 0.0361 lb/in³ | |
Nabaltec NABALOX® NO 713-10 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | 0.800 - 1.00 g/cc | 0.0289 - 0.0361 lb/in³ | |
Nabaltec NABALOX® NO 713-40 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | |
Invista 2201 PET Copolymer Packaging Resin
(discontinued **) Carboxyl end groups: |
|||
Bulk Density | 0.800 - 0.900 g/cc | 0.0289 - 0.0325 lb/in³ | PEPL-10-W-67 |
Pearl Engineering PEPLPET B-07C PET Bottle Grade A co-polymer used mostly for containers. |
|||
Bulk Density | 0.800 - 0.900 g/cc | 0.0289 - 0.0325 lb/in³ | PEPL-10-W-67 |
Pearl Engineering PEPLPET B-103C PET Bottle Grade A co-polymer used for mineral water bottles |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | DIN 53466 |
3M Dyneon™ PFA 6503 C EPC Perfluoroalkoxy Fluorothermoplastic
(discontinued **) Dyneon PFA 6503 C EPC is a fluorothermoplastic powder for powder coating applications, and is designed for thin film applications where target film thickness is 25-40 micrometers per pass.non-stick .. |
|||
Bulk Density | 0.800 - 1.05 g/cc | 0.0289 - 0.0379 lb/in³ | |
Magyar Aluminum ALO-DF223 Alumina Alumina for Polishing |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | Tap Density |
Momentive Performance Materials AC6001 Boron Nitride (BN) Powder Agglomerate of hexagonal BN crystals. AC6001 powders are granular with good flow and blend characteristics as well as high thermal conductivity and good lubrication qualities. Information provided.. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | ISO 60 |
Lanxess Pocan® T 7331 POS151 700226 PBT + PET, 30% Glass Fiber PBT + PET, 30% glass fibers, injection molding, improved surface finish, increased temperature peak load, UV stabilizedInformation provided by LANXESS. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | ISO 60 |
Lanxess Pocan® B 1701 000000 PBT PBT, non-reinforced, extrusion, food contactInformation provided by LANXESS. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | ISO 60 |
Lanxess Pocan® C 1202 000000 PET + PC PBT + PC, non-reinforced, injection molding, improved impact strength, low tendency to warp, UV-stabilizedInformation provided by LANXESS. |
|||
Bulk Density | 0.800 - 0.900 g/cc | 0.0289 - 0.0325 lb/in³ | |
Taiwan PU Corporation MOCA Polyurethane Resin Curing Agent MOCA [4,4' - Methylene bis-(ortho-chloroaniline)] is used as a PU curing agent. The chlorine atoms on benzene ring can slow down the activity of the NH2 group, so as to extend the pot life while ca.. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | ASTM D1895 |
Sumitomo Bakelite North America E 2748-9641D Short Glass Fiber Reinforced Epoxy E 2748-9641D is a mineral and short fiberglass filled epoxy molding compound.Information provided by Sumitomo Bak North America, Inc. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | ASTM D1895 |
Sumitomo Bakelite North America E 8354A-1 Short Glass Fiber Reinforced Epoxy E 8354A-1 is a fiberglass and mineral reinforced epoxy molding compound, with excellent dimensional stability, good electrical insulation properties, and good strength.Information provided by Sumito.. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | Powder; ISO 60 |
Sumitomo Bakelite North America RX® 611 Fiberglass Reinforced Phenolic RX 611 is a fiberglass reinforced phenolic molding compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type MFH.Information supplied by Sumitomo.. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | ASTM D1895 |
Sumitomo Bakelite Sumikon® PM-9501 Glass-Filled Phenolic, Compression Grade Sumikon PM-9501 is a two stage glass fiber and mineral filled black phenolic special purpose molding compound. It is especially designed for applications requiring high strength and dimensional s.. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | ASTM D1895 |
Sumitomo Bakelite Sumikon® PM-9501 Glass-Filled Phenolic, Injection Grade Sumikon PM-9501 is a two stage glass fiber and mineral filled black phenolic special purpose molding compound. It is especially designed for applications requiring high strength and dimensional s.. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | |
Solvay SUPRAGIL® RM/210 EI Polynaphthalenmethan-Sulphonate, Sodium Salt Description: Dispersing, non foaming agent.Identification: POLYNAPHTHALENMETHAN-SULPHONATE, SODIUM SALTCAS: 9084 – 06 – 4Solubility: Soluble in water. Insoluble in polar and aromatic solve.. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | Dry Density |
Zircar Ceramics AX Moldable Alumina-Silica Insulation AX Moldable is a sticky fiber rich paste useful to obtain a hard surface coating, bond alumina-silica fiber based insulation products to themselves and to form complex shapes for use to 1260°C (230.. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | ASTM D894 |
Daikin POLYFLON M-391 PTFE Molding Powder, Free Flow Free flow powder.Processing Methods: Compression molding and automatic or semi-automatic compression molding.Features: Used if concerned about insufficient molding pressure for flat sheets.Informati.. |
|||
Bulk Density | >= 0.800 g/cc | >= 0.0289 lb/in³ | |
Chosun Refractories B-4 Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | |
3M Dyneon™ Dynamar™ FX 9613 Polymer Processing Additive Dynamar polymer processing additive FX 9613 is a free flowing granular concentrate form of a fluoropolymer designed for use at very low levels to improve the processing of thermoplastics. At the ver.. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | DIN 53466 |
3M Dyneon™ PFA 6503PAZ Fluoroplastic Powder 3M™ Dyneon™ Fluoroplastic Powder PFA 6503PAZ is a fluorothermoplastic powder designed for use in thin film powder coatings. Typical applications include non-stick surfaces, chemical vessel and tan.. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | |
BASF Sicotan® Yellow K 1011 Color Additive Chemical Structure: Ni/Sb/Ti-oxideApplication: Colourant for plastics; PVC-p, PVC-u, LD-PE, HD-PE, PP, PS, SB, SAN, ABS/ASA, PMMA, PC, PA, PETP, CA/CAB and UPRecommendations for food applications: B.. |
|||
Bulk Density | 0.800 - 1.20 g/cc | 0.0289 - 0.0434 lb/in³ | |
Solvay Chemicals (CsAlF-Complex) Cesium Fluoroaluminate Low-melting-point flux for brazing aluminum.HS No.: 38109090 /CAS-No.: 138577-01-2 Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration and Household & Electrical Appl.. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | Powder; ASTM D1895 |
Sumitomo Bakelite North America FM 4005 Fiberglass Reinforced Phenolic Novolac FM 4005 is a fiberglass reinforced phenolic novolac molding compound, with excellent dimensional stability and good strength at elevated temperatures. This material is compliant with the specificat.. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | Powder; ASTM D1895 |
Sumitomo Bakelite North America FM 4017F Fiberglass and Mineral Reinforced Phenolic FM 4017F is a fiberglass and mineral reinforced phenolic molding compound, with excellent dimensional stability and good strength at elevated temperatures. Information supplied by Sumitomo Bak North.. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | DIN 53466 |
3M Dyneon™ PFA 6503 B EPC Perfluoroalkoxy Fluorothermoplastic
(discontinued **) Dyneon PFA 6503 B EPC is a fluorothermoplastic powder for powder coating applications, and is designed for thin film applications where target film thickness is 25-40 micrometers per pass.non-stick .. |