Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | <= 300 °C | <= 572 °F | |
Nabaltec APYMAG® 40 Magnesium Hydroxide The demand for halogen free flame retardant plastics for applications in automobile, electrical, and construction industries is stronger than ever. The use of mineral flame retardants within these p.. |
|||
Processing Temperature | 300 °C | 572 °F | Material Temperature |
Nanocyl PLASTICYL™ PC1501 Polycarbonate - Carbon Nanotube Masterbatch PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLA.. |
|||
Processing Temperature | 300 °C | 572 °F | Material Temperature |
Nanocyl PLASTICYL™ PC1501 Polycarbonate with 2 wt% Multi-Wall Carbon Nanotubes PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLA.. |
|||
Processing Temperature | 300 °C | 572 °F | Material Temperature |
Nanocyl PLASTICYL™ PA1501 Polyamide 66 with 2 wt% Multi-Wall Carbon Nanotubes PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLA.. |
|||
Processing Temperature | 300 °C | 572 °F | Material Temperature |
Nanocyl PLASTICYL™ PA1501 Polyamide 66 with 3 wt% Multi-Wall Carbon Nanotubes PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLA.. |
|||
Processing Temperature | 300 °C | 572 °F | Average value: 300 °C Grade Count:3 |
Overview of materials for Polycarbonate, Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Conductive". Each property range of values reported is minimum and maximum values of appr.. |
|||
Processing Temperature | <= 300 °C | <= 572 °F | |
Kingfa PC-S923 Modified PC Features:Excellent balance propertiesGood weather resistanceHigh impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile instrument panelElec.. |
|||
Processing Temperature | 300 - 380 °C | 572 - 716 °F | Hardening Temperature |
Möller Medical NanoSkin Magic 101 L NanoCoating Conducting coating with very good chemical resistance, biocompatible, becoming hydrophilic after water contactInformation provided by Möller Medical, Member of CENTROTEC Group |
|||
Processing Temperature | <= 300 °C | <= 572 °F | |
Kingfa CPA-6 Toughened PA6 Features:High impactLow tendency to wrapApplications:Injection moldingSport applianceAutomobile partsPower toolsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Processing Temperature | <= 300 °C | <= 572 °F | |
Kingfa PA6-M20G16 20% Glass & 16% Mineral Filled PA6 Features:Low tendency to wrapExcellent size stabilityLow abrasionOutstanding surfaceApplications:Injection moldingAutomobile partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Processing Temperature | <= 300 °C | <= 572 °F | |
Kingfa PA6-RG30 Flame Retardant, 30% Glass Fiber Reinforced PA6 Features:Flame retardantHigh strengthHigh temperature propertiesGood electric propertiesApplications:Injection moldingConnectorsRelayBobbinsPlugsInformation Provided by Kingfa Sci. & Tech. Co., Ltd... |
|||
Processing Temperature | <= 300 °C | <= 572 °F | |
DuPont™ Appeel® 22D843 Ethylene Acrylate DuPont™ Appeel® 22D843 is a polypropylene modified ethylene acrylate resin designed to function as a masterbatch to achieve peelability in polypropylene based sealant layers. It provides peelable .. |
|||
Processing Temperature | <= 300 °C | <= 572 °F | |
DuPont™ Fusabond® P613 Polymer Modifier DuPont™ Fusabond® P613 is a anhydride modified polypropylene. FUSABOND P613 resin conforms with the Code of Federal Regulations, Title 21, Paragraph 175.105, covering the use of adhesive interlay.. |
|||
Processing Temperature | <= 300 °C | <= 572 °F | |
Arkema Group LOTRYL® 18 MA 02 Copolymer Ethylene - Methyl Acrylate LOTRYL® 18 MA 02 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the methyl acrylate content, LOTRYL® 18 MA 02 is a polymer of .. |
|||
Processing Temperature | <= 300 °C | <= 572 °F | |
Arkema Group LOTRYL® 20 MA 08 Copolymer Ethylene - Methyl Acrylate LOTRYL® 20 MA 08 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the high methyl acrylate content, LOTRYL® 20 MA 08 is a polyme.. |
|||
Processing Temperature | <= 300 °C | <= 572 °F | |
Arkema Group LOTRYL® 24 MA 005 Copolymer Ethylene - Methyl Acrylate LOTRYL® 24 MA 005 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the high methyl acrylate content, LOTRYL® 24 MA 005 is a poly.. |
|||
Processing Temperature | <= 300 °C | <= 572 °F | |
Arkema Group LOTRYL® 28 BA 175 Copolymer Ethylene - Butyl Acrylate LOTRYL® 28 BA 175 is a random copolymer of ethylene and butyl acrylate, prepared by the high pressure polymerization process. Co-monomer content is 28% in weight. LOTRYL® 28 BA 175 is particularly.. |
|||
Processing Temperature | <= 300 °C | <= 572 °F | |
Arkema Group LOTRYL® 29 MA 03 Copolymer Ethylene - Methyl Acrylate LOTRYL® 29 MA 03 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the high methyl acrylate content, LOTRYL® 29 MA 03 is a polyme.. |
|||
Processing Temperature | <= 300 °C | <= 572 °F | |
Arkema Group LOTRYL® 35 BA 320 Copolymer Ethylene - Butyl Acrylate LOTRYL® 35 BA 320 is a random copolymer of ethylene and butyl acrylate, prepared by the high pressure polymerization process. Co-monomer content is 35% in weight. LOTRYL® 35 BA 320 is particularly.. |
|||
Processing Temperature | <= 300 °C | <= 572 °F | |
Arkema Group LOTRYL® 37 EH 175 Copolymer Ethylene - 2-Ethylhexyl Acrylate LOTRYL® 37EH175 is a random copolymer of Ethylene and 2-Ethylhexyl Acrylate, prepared by the high pressure polymerization process. LOTRYL® 37EH175 is particularly recommended for the formulation o.. |
|||
Processing Temperature | <= 300 °C | <= 572 °F | |
Addcomp ADD-MAX® 804 Efficiency masterbatch, PET based Fields of application: Masterbatch for improvement of production efficiency and product quality.Examples: PET cast and blown films, pipes, tubes, wire and cables, blow moulding and general extrusion.. |
|||
Processing Temperature | <= 300 °C | <= 572 °F | |
Addcomp ADD-VANCE® CL 622 Nucleation masterbatch, PP based Fields of application: Injection molded, extruded and thermoformed articles made from PP resins.Examples: Injection molded, extruded and thermoformed articles made from PP resins. Mode of action and.. |
|||
Processing Temperature | <= 300 °C | <= 572 °F | |
Addcomp ADD-VANCE® DS 485 Desiccant masterbatch in LLDPE carrier Fields of application: Highly concentrated desiccant masterbatch for LDPE, LLDPE, HDPE, PP, EVA and other ethylene copolymers.Examples: Elimination of moisture from (recycle) polymers in moisture se.. |
|||
Processing Temperature | <= 300 °C | <= 572 °F | |
Addcomp ADD-MAX® 182 Efficiency masterbatch Fields of application: Improvement of production efficiency and product qualityExamples: Polyamide 6 and 6,6 staple fibers produced on “short spin” lines.Mode of action and advantages: ADD-MAX 182.. |
|||
Processing Temperature | 300 - 320 °C | 572 - 608 °F | Hardening Temperature |
Möller Medical NanoSkin Magic 112 NanoCoating Thermal resistant coating with outstanding easy-to-clean effect and chemical resistance, bioinertInformation provided by Möller Medical, Member of CENTROTEC Group |
|||
Processing Temperature | <= 300 °C | <= 572 °F | |
Addcomp ADD-VANCE® NU 559 Nucleation masterbatch, PP based Fields of application: Extruded and injection molded articles made from PP and PE resins.Examples: Extruded sheets, films, tapes and blow molded, compression molded and injection molded articles, su.. |
|||
Processing Temperature | <= 300 °C | <= 572 °F | |
PolyChem Alloy PolyGard 7507N PolyFoam decomposes when heated to create a uniform microcellular structure. It can be used in extrusion and injection molding processes to reduce weight in parts without adversely affecting the ph.. |